Description
Product Overview
The Thorlabs PF03-03-M02 is a Ø7.0 mm plano mirror with a mid-infrared enhanced gold coating on a fused silica substrate, specified for 2 to 20 µm at above 98% average reflectance and above 95% absolute reflectance over an angle of incidence from 0 to 45 degrees. It is the mid-infrared specialist of the PF03-03 series, and the distinction it draws is narrow but real.
A protected gold mirror is a broadband compromise. The dielectric overcoat that makes the gold durable also introduces absorption that grows toward the longer wavelengths, and the effect that is negligible at 1 µm becomes measurable at 10 µm. The mid-infrared enhanced coating changes that balance: the overcoat is designed so that its losses sit outside the 2 to 20 µm band, which is how the average reflectance reaches 98% where protected gold reaches 96%. The overcoat is qualified to MIL-C-48497A, so the gain in reflectance is not bought with durability, and the mirror remains cleanable.
The improvement past 2 µm is paid for below it. The same overcoat that is transparent in the mid infrared costs reflectance in the near infrared, and Thorlabs states the trade explicitly: these mirrors perform worse than protected gold below 2 µm. That is the reason both coatings exist in the same family and the same mount, and the reason the choice between them is a wavelength decision rather than a quality decision.
The substrate is fused silica, 2.0 mm thick, with flatness better than λ/10 peak to valley at 633 nm, 40-20 scratch-dig surface quality and parallelism within 3 arcmin. The clear aperture is over Ø6.3 mm. At Ø7.0 mm the mirror fits the MK7 mini-series mount and the LMR7 fixed mount, which is what makes it usable as the small turning mirror in a multi-pass gas cell or a compact sensor head.
Key Features
- Mid-infrared enhanced gold coating: average reflectance above 98% and absolute reflectance above 95% from 2 to 20 µm, over an incidence range of 0 to 45 degrees
- Overcoat qualified to MIL-C-48497A: the durability of a protected coating with the reflectance of an enhanced one, so the mirror can be handled and cleaned
- Fused silica substrate: λ/10 peak-to-valley figure at 633 nm, 40-20 scratch-dig surface quality, parallelism within 3 arcmin, clear aperture over Ø6.3 mm
- Ø7.0 mm x 2.0 mm: fits the MK7 and MK7/M mini-series mount and the LMR7 and LMR7/M fixed mount, small enough for a multi-pass cell or a sensor head
- Published damage thresholds: 0.1 J/cm² for 10 ns pulses at 1.064 µm and 3 J/cm² for 100 ns pulses at 10.6 µm, with 25 W/cm and 450 W/cm continuous figures at the same wavelengths
- Cleanable: solvent and tissue cleaning are permitted, which matters because mid-infrared optics are usually installed by hand in open setups
Technical Specifications
| Model | PF03-03-M02 |
| Coating | Mid-infrared enhanced gold, overcoat per MIL-C-48497A |
| Wavelength range | 2 µm – 20 µm |
| Average reflectance | above 98% from 2 to 20 µm |
| Absolute reflectance | above 95% from 2 to 20 µm |
| Angle of incidence | 0 to 45 degrees |
| Substrate | Fused silica |
| Diameter | Ø7.0 mm |
| Diameter tolerance | +0.0 mm / -0.1 mm |
| Thickness | 2.0 mm (0.08 in) |
| Thickness tolerance | +/-0.2 mm |
| Clear aperture | over Ø6.3 mm |
| Front surface flatness | λ/10 peak to valley at 633 nm |
| Surface quality | 40-20 scratch-dig |
| Parallelism | at most 3 arcmin |
| Pulsed damage threshold | 0.1 J/cm² at 1.064 µm (10 ns, 10 Hz, Ø1.06 mm); 3 J/cm² at 10.6 µm (100 ns, 1 Hz, Ø1.29 mm) |
| CW damage threshold | 25 W/cm at 1.070 µm; 450 W/cm at 10.6 µm |
| Mount compatibility | MK7 / MK7/M mini-series mount, LMR7 / LMR7/M fixed mount |
| Cleanable | Yes |
Source: Thorlabs official product page and family specification table. Values are for the Ø7.0 mm item; other diameters in the same family differ in thickness and clear aperture.
Applications
The coating is chosen where the working wavelength sits above 2 µm and the reflectance matters, which in practice means sensing and thermal work rather than general beam routing.
- Gas sensing with quantum cascade and interband cascade lasers, where the source power is low and a two percentage point gain in reflectance across several folds is worth having
- Mid-infrared supercontinuum sources, where the beam is broadband and a coating with structure in the band would impose that structure on the measurement
- Multi-pass absorption cells, where the small turning mirrors that steer a beam into and out of the cell are exactly this size and exactly this band
- Thermal imaging and radiometry from 2 to 20 µm, where the mirror has to be cleanable because it is installed in an open instrument
- 10.6 µm CO2 laser work, where the higher reflectance and the 3 J/cm² pulsed threshold at that wavelength both matter
- FTIR accessories and infrared microscope paths, where the optic is handled during alignment and a bare gold film would not survive the handling
Selection Guide
- Decide by the short-wavelength end of the band: if the beam never goes below 2 µm, this coating is the best of the three. If the path also carries near-infrared light, protected gold covers 800 nm to 20 µm and performs better below 2 µm, at the cost of about two percentage points in the mid infrared
- Use the absolute reflectance figure where the budget is tight: the average is above 98%, the absolute minimum is above 95%. A multi-pass cell multiplies whichever figure applies, so the absolute number is the one to put into a throughput calculation
- Check the angle range against the layout: the specification covers 0 to 45 degrees of incidence. A layout that folds the beam beyond 45 degrees is outside the published range and needs a curve rather than an assumption
- Check continuous power in W/cm of beam diameter: the 450 W/cm figure at 10.6 µm is a linear power density, so it is the beam diameter rather than the area that goes into the calculation
- Confirm the mount: Ø7.0 mm optics use the MK7 mini-series or the LMR7 fixed mount, both sized for a 2 mm substrate
Series Comparison
The three Ø7.0 mm mirrors in this group share a substrate, a figure and a mount, and differ in coating. This page is the mid-infrared option, and it is the one to choose when the working band starts at 2 µm rather than at 800 nm.
| Model | Coating | Wavelength range | Average reflectance | Cleanable | Typical use |
| PF03-03-F01 | UV-enhanced aluminum | 250 nm – 450 nm | over 90% | No | UV and blue beam steering, harmonics, fluorescence excitation |
| PF03-03-M01 | Protected gold | 800 nm – 20 µm | over 96% | Yes | Broadband infrared folding, CO2 laser delivery, general IR work |
| PF03-03-M02 – this page | Mid-infrared enhanced gold | 2 µm – 20 µm | over 98% | Yes | Mid-infrared sensing, thermal imaging, 10.6 µm processes |
The wider family shows where the boundaries fall. The same substrate standard carries six coatings, so a wavelength change is met by changing the suffix rather than the mechanical design.
| Coating | Wavelength range | Average reflectance | Cleanable | Where it is used |
| UV-enhanced aluminum | 250 nm – 450 nm | over 90% | No | Ultraviolet and blue beam steering where a metal coating is wanted |
| Protected aluminum | 450 nm – 2 µm (over 90%); 2 – 20 µm (over 95%) | over 90% / over 95% | Yes | General broadband folding at low cost, visible to mid-infrared |
| Protected silver | 450 nm – 2 µm (over 97.5%); 2 – 20 µm (over 96%) | over 97.5% / over 96% | Yes | Highest visible and near-infrared reflectance, broadband |
| Protected gold | 800 nm – 20 µm | over 96% | Yes | General infrared folding, CO2 laser beam delivery |
| MIR-enhanced gold | 2 µm – 20 µm | over 98% | Yes | Mid-infrared sensing, thermal imaging, 10.6 µm work |
| Unprotected gold | 800 nm – 20 µm | over 97% | No | Highest gold reflectance where the optic is never touched |
Usage Precautions
- Handling: wear finger cots or powder-free gloves and hold the mirror by its rim. The overcoat resists abrasion but not the oils in a fingerprint, and an optic installed with a contaminated face will lose reflectance where the beam passes
- Cleaning: cleaning is permitted. Blow off loose dust, then drag a lens tissue moistened with solvent across the surface in one direction and finish with a dry drag. Do not scrub, and do not reuse a tissue
- Storage: keep the mirror in its case in a dry environment. The overcoat is a dielectric layer, and humid storage attacks it at pinholes rather than uniformly, so the loss appears as scatter rather than as a drop in reflectance
- Mounting: tighten the retaining ring only until the optic is held. A 2 mm substrate distorts under clamping force, and the λ/10 figure is lost before alignment begins
- Optical power: compare the linear power density of the beam with the CW figure for the wavelength in use, and the energy density with the pulsed figure for the actual pulse length. At 10.6 µm the pulsed and continuous figures differ by more than an order of magnitude, so using the wrong one is a real risk
- Alignment and back reflection: keep the beam inside the clear aperture and tilt the mirror slightly off normal where the layout allows, so the reflection does not return into the source. At mid-infrared power levels a returned beam is a hazard as well as a source of instability
FAQ
How does mid-infrared enhanced gold differ from protected gold? Both are gold films under a dielectric overcoat and both can be cleaned. The M02 overcoat is designed so that its absorption sits outside the 2 to 20 µm band, which lifts average reflectance to above 98% against above 96% for protected gold. The same design costs reflectance below 2 µm, where protected gold performs better. The choice follows the working wavelength.
Can the PF03-03-M02 be cleaned? Yes. The overcoat is qualified to MIL-C-48497A and is intended to survive normal handling and cleaning. Blow off loose contamination, then use a solvent-moistened lens tissue in a single direction and finish dry.
Why is the pulsed threshold so much lower at 1.064 µm than at 10.6 µm? Because the two figures are measured with different pulse lengths. The 0.1 J/cm² value is for 10 ns pulses at 1.064 µm and the 3 J/cm² value is for 100 ns pulses at 10.6 µm. Energy density scales roughly with the square root of pulse length for nanosecond pulses, so the two numbers are not directly comparable; use the figure measured at the wavelength and pulse length closest to your own.
Which mount takes a Ø7.0 mm mirror? The MK7 and MK7/M mini-series mount and the LMR7 and LMR7/M fixed mount, both sized for a 7 mm optic with a 2 mm substrate.
Is the coating suitable below 2 µm? Not as the first choice. The overcoat that improves performance past 2 µm causes performance to suffer in the near infrared, and the protected gold mirror in the same family is the better option there.
Disclaimer
Specifications on this page are compiled from Thorlabs official published material and are provided as a selection reference. The current official specification sheet governs; specifications and appearance may change without notice. Price and lead time are quoted by our sales team on request. Reproduction of this page without written permission is not permitted.
About the Brand
Thorlabs is a manufacturer of photonics and optical components. The metal-coated plano mirrors in the PF03-03 series are produced at the company’s coating facility in Newton, New Jersey, and the range covers UV-enhanced aluminum, protected aluminum, protected silver, protected gold, mid-infrared enhanced gold and unprotected gold on the same substrate and the same mounting standard. That common platform is the practical value of the series: a design can change coating to follow a wavelength change without changing the mount, the clear aperture or the optical axis. Figure, surface quality, parallelism and laser damage threshold are published per coating and per diameter rather than as one figure for the family, which is why the tables on this page are specific to the Ø7.0 mm item.
Selection enquiries: Changsha Soar Laser Equipment Co., Ltd., hotline +86 159 2722 0467, www.soar-laser.cn, email 859818709@qq.com.









Reviews
There are no reviews yet.