QQ: 859818709

Thorlabs PF2011-P01 Ø50.8 mm (2 in) Zerodur® Protected Silver Mirror, 450 nm – 20 µm

Thorlabs PF2011-P01 Ø50.8 mm (2 in) Zerodur® Protected Silver Mirror, 450 nm – 20 µm

Price on request
Category:

Description

Thorlabs PF2011-P01 Ø50.8 mm (2 in) Zerodur® Protected Silver Mirror, 450 nm – 20 µm

Product Overview

There is a particular kind of purchasing decision in which the best optical performance and the worst environmental tolerance arrive in the same box. The PF2011-P01 is that box. Silver is, by a clear margin, the most reflective metal available for the visible and near infrared, and it is also the only common coating metal that is chemically attacked by trace sulphur compounds and by moisture. Putting it on a Zerodur® body solves the thermal problem completely and does nothing at all about the chemical one. Understanding which of the two problems you have just bought is the whole of specifying this part correctly.

The numbers first. This is a round mirror 50.8 mm (2 in) in diameter and 12.0 mm (0.47 in) thick, Zerodur® substrate, protected silver coating behind a SiO₂ overcoat roughly 100 nm thick, specified from 450 nm to 20 µm with an average reflectance of 97 percent from 450 nm to 2 µm and 95 percent from 2 to 20 µm. Front surface flatness is λ/10 at 632.8 nm, surface quality is 40-20 scratch-dig, clear aperture is 45.7 mm, parallelism is 3 arcmin or better, incidence angles from 0° to 45° are specified, and the model number is laser-engraved on the fine-ground back face. Thorlabs states the design position plainly: in the visible to near-infrared spectral range, silver mirrors are the highest-reflectance metallic mirrors, and they also offer high reflectance in the infrared.

Seven percentage points sounds like a small number until it is multiplied by the number of times the beam hits a mirror. Take a six-fold relay, which is unremarkable in a spectroscopy bench or a laser processing head, and compare this coating with the protected aluminum alternative on the same body. At an average of 97 percent per bounce, six bounces leave 83.3 percent of the input power, a loss of 16.7 percent. At 90 percent per bounce, six bounces leave 53.1 percent, a loss of 46.9 percent. The silver path delivers 1.57 times the power at the sample. Whether that factor matters depends entirely on what is downstream: for a camera that is already near saturation it is irrelevant, and for a photon-starved measurement or a fixed laser budget it is the difference between a working experiment and a longer integration time.

The step from 97 percent to 95 percent at 2 µm is not a defect; it is where silver’s behaviour changes. Silver is an excellent reflector through the visible and near infrared, and in the mid infrared the free-electron response still gives high reflectance but the finite conductivity and the surface quality of the metal begin to cost a little. The two figures are averages over two intervals of very different width, 1.55 µm and 18 µm, and each applies only inside its own interval.

The 100 nm overcoat deserves its own paragraph because it is the most misunderstood feature of the part. A layer that thin cannot be a mechanical shield, and it is not intended to be. Its job is chemical: it keeps oxygen and sulphur-bearing species away from the silver surface, which is what stops the film from tarnishing. It happens also to be optically active. For a silicon dioxide index near 1.45, a 100 nm film is close to a quarter-wave optical thickness at about 580 nm, which means this very thin layer still shifts the phase and the polarization of the reflected beam in the visible, in a way that depends on angle. That is a real effect and it is the reason the overcoat is described as a protection rather than as an optical element: it is a compromise between chemical isolation and optical neutrality, resolved in favour of the thinnest layer that still works.

And then the sentence that decides where this mirror may be installed. Thorlabs states that while the protective coating prevents the silver from oxidizing, it should not be used in high-humidity environments. That is not a caution about condensation on a cold optic; it is a statement about the coating’s chemistry. Silver mirrors are unusually sensitive to their environment and to improper handling, and fingerprints, contact with abrasive surfaces, high humidity and high temperature all reduce the effectiveness of the protective coating and leave the silver free to oxidise and degrade. The recommended practice is to wear latex gloves, and even with that protection not to touch the mirror surface or its edges, and to use and store the part at room temperature in a low-humidity environment. Read those instructions as installation requirements, not as suggestions.

Zerodur is a registered trademark of Schott.

Bounces in the relay Protected silver at 97% per bounce Protected aluminum at 90% per bounce Ratio
2 94.1% 81.0% 1.16
4 88.5% 65.6% 1.35
6 83.3% 53.1% 1.57

These are band averages compounded arithmetically, which is an approximation: the actual value at your wavelength may be a little above or below the average, and any window, filter or lens in the same path adds its own loss. The table is there to show the shape of the compounding, not to replace a link budget.

Key Features

  • The highest reflectance of any metallic coating in the visible and near infrared. Average 97 percent from 450 nm to 2 µm, which is the figure that most optical designs are actually trying to reach when they start considering dielectric stacks and then discover the cost and the angular sensitivity.
  • Still 95 percent average from 2 to 20 µm. The same optic covers a CO₂ line and a thermal imaging band without changing coatings, which is unusual for a coating that is optimised for the visible.
  • SiO₂ overcoat approximately 100 nm thick. Thin enough to stay optically close to neutral, thick enough to keep oxygen and sulphur species off the silver. The thickness is the compromise, and it is why this part is not simply “silver with a protective layer”.
  • Zerodur® substrate at 0 ± 0.100 x 10⁻⁶/°C. The best reflectance in the family on the most dimensionally stable body in the family, which is exactly the combination a high-power visible or near-infrared system needs: maximum delivered power and minimum thermal pointing drift.
  • Four published damage thresholds covering femtosecond, nanosecond and continuous operation. 0.225 J/cm² at 800 nm with 99 fs pulses at 1 kHz over a Ø0.167 mm spot, 1 J/cm² at 1064 nm with 10 ns pulses at 10 Hz over a Ø1.010 mm spot, 500 W/cm at 1.07 µm over a Ø0.974 mm spot and 1500 W/cm at 10.6 µm over a Ø0.339 mm spot. This is the most complete damage data set in the family, and it is the only one with a femtosecond measurement.
  • λ/10 at 632.8 nm, 40-20 scratch-dig, 45.7 mm clear aperture, 3 arcmin parallelism. The figure is what makes the high reflectance usable in an imaging or interferometric path rather than only in a beam dump.
  • Not for humid environments. Stated by the manufacturer, and repeated here because it is the single specification most often ignored when a part is transferred from one laboratory to another.

Technical Specifications

Parameter Specification
Part Number PF2011-P01
Coating Protected silver
Overcoat SiO₂, approximately 100 nm thick
Spectral Range 450 nm to 20 µm
Average Reflectance, Visible to SWIR Ravg of 97 percent from 450 nm to 2 µm
Average Reflectance, Mid to Far IR Ravg of 95 percent from 2 to 20 µm
Substrate Zerodur® (substrate grade)
Coefficient of Thermal Expansion 0 ± 0.100 x 10⁻⁶/°C (fused silica reference: 0.55 x 10⁻⁶/°C)
Diameter 50.8 mm (2 in), tolerance +0.0 / -0.1 mm
Thickness 12.0 mm (0.47 in), tolerance ±0.2 mm
Parallelism 3 arcmin or better
Front Surface Flatness λ/10 at 632.8 nm
Surface Quality 40-20 scratch-dig
Clear Aperture 90 percent of diameter (45.7 mm)
Angle of Incidence 0° to 45°
Back Surface Fine ground, model number laser-engraved
Pulsed Damage Threshold (femtosecond) 0.225 J/cm² at 800 nm, 99 fs, 1 kHz, Ø0.167 mm
Pulsed Damage Threshold (nanosecond) 1 J/cm² at 1064 nm, 10 ns, 10 Hz, Ø1.010 mm
CW Damage Threshold (1.07 µm) 500 W/cm at 1.07 µm, Ø0.974 mm
CW Damage Threshold (10.6 µm) 1500 W/cm at 10.6 µm, Ø0.339 mm
Environmental Restriction Not for use in high-humidity environments
Handling Latex gloves; do not touch the mirror surface or the edges

The four damage thresholds are the most useful part of this table and the most easily misread. They are not four points on one curve. They come from four different test campaigns with different wavelengths, pulse durations, repetition rates and spot sizes, and the only way to use them is to convert each one into the quantity it actually represents for a beam of that shape.

Test Published value Spot What that is in absolute terms
800 nm, 99 fs, 1 kHz 0.225 J/cm² Ø0.167 mm About 49 µJ in a single pulse at that spot
1064 nm, 10 ns, 10 Hz 1 J/cm² Ø1.010 mm About 8 mJ in a single pulse at that spot
1.07 µm, CW 500 W/cm Ø0.974 mm About 49 W of incident power, near 6,500 W/cm²
10.6 µm, CW 1500 W/cm Ø0.339 mm About 51 W of incident power, near 56,000 W/cm²

Look at the two CW rows together. The linear power density differs by a factor of three, but the absolute power is almost identical, about 49 W against about 51 W, and the intensity differs by a factor of 8.6 because the spot sizes differ by a factor of 2.9. This is not a contradiction in the data; it is a demonstration that a CW threshold quoted in W/cm is a convention tied to a test geometry, and the geometry changes between the two measurements. The far-infrared test is far harsher per unit area than the near-infrared one. Anyone who reads 1500 W/cm as three times more capability at 10.6 µm has read the units and missed the geometry.

Applications

  • Photon-starved spectroscopy with multiple folds. When the signal is a handful of counts and the beam path folds four or six times, seven percentage points per bounce is the largest single improvement available without changing the source.
  • Laser scanning and confocal microscopy. Silver’s reflectance across the visible keeps the excitation and the emission band equally well served, and the λ/10 figure keeps the scan lens input wavefront clean.
  • High-power visible and near-infrared delivery with thermal stability. The combination of the highest reflectance in the family with a substrate at 0 ± 0.100 x 10⁻⁶/°C is aimed at systems where both delivered power and pointing stability are specified.
  • Femtosecond oscillator and amplifier folding. This is the only coating in the family with a published femtosecond threshold, 0.225 J/cm² at 800 nm with 99 fs pulses, which makes it the one that can be specified for an ultrafast path without a qualification run, provided the pulse energy stays well inside that figure.
  • Mid-infrared beam combining. A 95 percent average from 2 to 20 µm lets a visible alignment beam and an infrared working beam share a fold, which is otherwise a dichroic design problem.
  • Interferometry and wavefront sensing in the visible. The 45.7 mm clear aperture and the λ/10 figure support a two-inch beam, and the high reflectance keeps the reference arm bright.

Selection Guide

The choice between silver and aluminium on this body is decided by two questions, in this order. First: does the environment permit silver at all? If the optic will live in an unheated room, near a water bath, in a coastal building, or in a housing that is opened to laboratory air, the answer is aluminium, and the seven percentage points are irrelevant because the silver will not survive long enough to deliver them. Thorlabs is explicit that the protective overcoat does not make the mirror suitable for high humidity, and no amount of careful handling changes the chemistry.

Second: is the beam visible or near infrared, and does the power budget matter? If the answer to both is yes, silver is the correct coating and aluminium is the compromise. If the beam is at 10.6 µm and the power budget matters, silver’s 95 percent average over 2 to 20 µm is competitive with aluminium’s 95 percent over the same interval, and the decision moves to damage threshold and environment rather than to reflectance. If the beam is below 450 nm, neither coating applies and the UV-enhanced part is the only option in the family.

On geometry, the clear aperture is 45.7 mm and the specified incidence range runs to 45°, where the footprint stretches by about 1.41 in one axis. A two-inch optic is the right size for a beam up to roughly 30 mm at 45°, which is the usual reason this diameter is chosen over the one-inch part for an expanded beam. Mount it with a compliant retainer bearing outside the clear aperture, and never let a metal retaining ring contact the coating: the edge of a silver mirror is the place where the overcoat is thinnest and where handling damage begins.

Series Comparison

Seven metallic coatings share this body. For this page the interesting columns are the two reflectance intervals and the environmental tolerance, because those are what separate silver from everything else.

Code Coating Spectral Range Average Reflectance Overcoat Environmental Note
F01 UV-enhanced aluminum 250-450 nm Ravg 90% MgF₂ Clean by displacement only
G01 Protected aluminum 450 nm-20 µm Ravg 90% (450 nm-2 µm), 95% (2-20 µm) SiO₂ More tolerant of humidity than silver
P01 Protected silver 450 nm-20 µm Ravg 97% (450 nm-2 µm), 95% (2-20 µm) SiO₂, approx. 100 nm Not for high humidity
M01 Protected gold 800 nm-20 µm Ravg 96% SiO₂ Chemically inert metal
M02 MIR enhanced gold 2-20 µm Ravg 98% SiO₂ Chemically inert metal
M03 Unprotected gold 800 nm-20 µm Ravg 97% None Not cleanable
L01 Unprotected gold, line optimised 10.6 µm line Ravg 99% None Not cleanable

The table makes the trade visible in one line. Silver is the only coating that reaches 97 percent in the visible interval, and it is the only coating in the family carrying an explicit environmental prohibition. Aluminium, one row above, gives up seven points in the visible and gains the right to be installed almost anywhere. Gold, further down, is chemically inert and reaches 96 percent in the infrared but cannot help below 800 nm. There is no row that combines silver’s visible reflectance with gold’s indifference to its environment, which is why the choice between them is a decision about the room, not about the optics.

FAQ

Q1. Some listings give ninety-seven point five percent for this coating and your page gives 97 percent. Which is right?

The single-item specification for the protected silver coating in this family is an average of 97 percent from 450 nm to 2 µm and 95 percent from 2 to 20 µm, and those are the figures this page uses. A value in the high nineties that ends in a half sometimes appears in multi-piece listings, in summaries that quote a peak rather than an average, and in third-party pages that have copied one another. The half-point difference is small, but the practice of quoting a peak as if it were an average is not: an average is what a link budget needs, because it describes the whole band rather than the best wavelength inside it. Use the 97 percent and 95 percent banded averages from the single-item specification, and if you need the value at one specific wavelength, ask for the measured curve.

Q2. How much does the environment actually matter for a protected silver mirror?

Enough that the manufacturer states the restriction explicitly. The overcoat prevents oxidation in normal conditions, but the part should not be used in a high-humidity environment, and the reason is that the failure is cumulative rather than sudden. Moisture and sulphur-bearing species reach the silver through pinholes and at the coating edge, the silver sulphides or oxidises, and the result is a slow loss of reflectance that starts at the edges and works inward. Nothing in the optical specification will warn you: the mirror looks fine and the throughput quietly drops over months. If the installation cannot be kept dry, specify aluminium instead and accept the seven points.

Q3. Is a 100 nm overcoat thick enough to protect the silver?

It is thick enough to do the job it was designed for, which is to keep oxygen and sulphur species away from the metal under normal laboratory conditions, and it is deliberately thin so that it stays optically close to neutral. It is not a mechanical shield and it is not a hermetic seal. A 100 nm film can be damaged by a tissue dragged across it, and it can be bypassed by water given enough time and enough cycling. The protection is a compromise between chemistry and optics, and the handling rules exist because the compromise is a narrow one.

Q4. The femtosecond threshold is 0.225 J/cm². Is that high or low?

For a metal coating with a dielectric overcoat it is a realistic working figure rather than a generous one, and it is measured at a small spot, Ø0.167 mm, which corresponds to about 49 µJ in a single 99 fs pulse. The important thing about a femtosecond threshold is that it is a measurement at one pulse duration and one repetition rate: the damage mechanism is electronic rather than thermal, so the value does not scale with pulse energy the way a nanosecond threshold does. If your pulse is 50 fs or 300 fs, or your repetition rate is 100 kHz rather than 1 kHz, the number you should design to is not this one.

Q5. Can I clean a silver mirror with the usual solvent and tissue routine?

Only with great care, and only if there is something on the surface that has to come off. The recommended practice from the manufacturer is to wear latex gloves and not to touch the mirror surface or the edges even with that protection, which tells you how the coating responds to contact. If cleaning is unavoidable, flood with clean solvent, drag a lens tissue once in one direction under its own weight, and stop. Never rub, never use a dry tissue, and never touch the edge, where the coating is most exposed.

Q6. Why does the reflectance fall from 97 to 95 percent at 2 µm?

Because silver’s reflectance is not perfectly flat: it is very high through the visible and near infrared and declines gradually as the wavelength lengthens, as the metal’s finite conductivity and surface scattering begin to matter more. The specification changes its average at 2 µm because that is where the behaviour changes enough to warrant a second number. It is not a coating defect and it is not a step in the curve at exactly 2 µm; it is two averages taken over two intervals of very different width, and the boundary between them is a reporting convention rather than a physical edge.

Usage Precautions

  • Wear latex gloves and do not touch the surface or the edges. This is the manufacturer’s recommendation and it is more specific than the usual glove advice: the edge of a silver mirror is where the coating terminates and where contamination begins.
  • Keep the part out of high humidity, permanently. Not just during storage. Use it at room temperature in a low-humidity environment, and if the housing is purged, keep the purge running whenever the optic is in use.
  • Do not place a silver mirror where it will see condensation cycles. A cold optic brought into a warm room, a water-cooled housing, or an enclosure that is opened to humid air will accumulate moisture on the coating, and the overcoat will not stop it.
  • Keep abrasives away from the coating and the edge. Fingerprints, contact with abrasive surfaces, high humidity and high temperature all reduce the effectiveness of the protective coating, which is exactly the list the manufacturer gives for what makes silver degrade.
  • Mount with a compliant retainer outside the clear aperture. Metal on glass at the rim is the classic way a coated edge gets chipped, and a chipped edge on a silver mirror is an entry point for the atmosphere.
  • Store in the case, at room temperature, in a dry place. Do not store a silver mirror in a sealed container with foam that can outgas, and do not leave it in a mount on an open bench for long periods.

Disclaimer

The specifications on this page are compiled from Thorlabs’ publicly published product documentation and are provided for selection reference only. Where this page differs from the manufacturer’s current official datasheet, the datasheet prevails. Coatings, specifications and appearance may change without notice. Damage thresholds are measured values under the stated test conditions and are not a guarantee of performance in any particular setup; users are responsible for verifying suitability at their own wavelength, fluence, pulse duration, repetition rate and beam size. The throughput and intensity conversions on this page are arithmetic from published figures, not manufacturer specifications. Prices and lead times are confirmed by our sales team at quotation.

Contact Us

Tell us the environment first and the reflectance requirement second. If the installation is dry and the beam is visible or near infrared, silver is almost certainly the right answer and we will quote it. If the installation is humid, we will tell you so before you buy, because a silver mirror in the wrong room is an expensive way to learn about chemistry.

Hotline: +86 159-2722-0467

E-mail: 859818709@qq.com  |  Website: www.soar-laser.cn

Evaluation units and volume orders are both available, and the same protected silver coating can be quoted in Ø1/2 in and Ø1 in bodies where the beam does not need a two-inch aperture.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF2011-P01 Ø50.8 mm (2 in) Zerodur® Protected Silver Mirror, 450 nm – 20 µm”

Your email address will not be published. Required fields are marked *