Description
Product Overview
The PF10-03-M03 is bare gold on fused silica: a Ø25.4 mm disc, 6.0 mm thick to within plus or minus 0.2 mm, with a gold film and nothing over it, specified at 97 percent average reflectance from 800 nm to 20 µm at incidence angles from 0 to 45 degrees. The front face is figured to λ/10 at 633 nm, surface quality is 40-20 scratch-dig, parallelism is 3 arcmin or better, the clear aperture is 90 percent of the diameter at Ø22.9 mm, and the rear face is fine ground and engraved with the item number.
Two consequences follow from the absence of an overcoat, and between them they are the entire argument for specifying this part. The first is reflectance. Between 800 nm and 2 µm the bare film is the brightest surface in the family at 97 percent, a full point above protected gold and well above protected aluminium, and it holds that level across the whole 20 µm band. The second is that nothing sits between the gold and the beam. There is no dielectric layer to introduce the polarization change that the manufacturer itself describes as difficult to quantify on protected gold, and no overcoat absorption in the mid to far infrared.
That combination makes this the standard choice for polarization-sensitive paths: a polarizing interferometer, the final fold of a polarization-maintaining delivery fibre, an ellipsometer, a Fresnel reflection experiment where the reflected state is the measurement. It is also the usual choice for ultrafast work, where an overcoat would add dispersion to a pulse that the rest of the system was designed to preserve. And because bare gold absorbs almost nothing at long wavelengths, it carries the highest continuous rating in the family at 10.6 µm, 1000 W/cm.
The handling protocol is not advice attached to the end of the datasheet. It is the operating condition of the part. A protected mirror that is mishandled can be cleaned; this one cannot, and a single fingerprint in the wrong place converts a usable optic into a rejected one. Read the precautions below before the mount comes off the bench, not after the optic is already in it.
Key Features
- No overcoat, no polarization penalty: the reflected polarization state is not altered by a dielectric stack, which is the reason this coating exists alongside protected gold
- 97 percent average reflectance, 800 nm to 20 µm: the highest in the family between 800 nm and 2 µm, and flat enough to serve a multi-band path
- 1000 W/cm continuous at 10.6 µm: the highest continuous rating of any metal coating here, because there is no overcoat to absorb
- 4 J/cm² pulsed at 10.6 µm: measured with 100 ns pulses at 1 Hz over a 0.435 mm spot, which is a demanding test for a bare film
- No dispersion from an overcoat: relevant to femtosecond and picosecond paths where every extra layer adds to the group delay
- λ/10 at 633 nm, 40-20 scratch-dig: a wavefront good enough for interferometry, not only for beam steering
- 6.0 mm fused silica: dimensionally stable, and thick enough that a correctly loaded ring does not distort the figure
- Engraved item number on the rear: identification without touching the coated face, which matters more here than anywhere else in the range
Technical Specifications
| Model | PF10-03-M03 |
| Coating | Unprotected gold (bare gold film, no dielectric overcoat) |
| Wavelength range | 800 nm – 20 µm |
| Average reflectance | Ravg over 97 percent across the full band |
| Angle of incidence | 0 to 45 degrees |
| Substrate | Fused silica |
| Diameter | Ø25.4 mm (1 inch) |
| Diameter tolerance | +0.0 mm / -0.1 mm |
| Thickness | 6.0 mm (0.24 in) |
| Thickness tolerance | plus or minus 0.2 mm |
| Surface flatness | λ/10 at 633 nm, peak to valley |
| Surface quality | 40-20 scratch-dig |
| Parallelism | 3 arcmin or better |
| Clear aperture | 90 percent of diameter (Ø22.9 mm) |
| Rear surface | Fine ground, laser engraved with the item number |
| Damage threshold, pulsed | 4 J/cm² at 10.6 µm (100 ns, 1 Hz, Ø0.435 mm) |
| Damage threshold, CW | 1000 W/cm at 10.6 µm (Ø1.18 mm) |
| Cleaning | Dry air or nitrogen blow-off only; no solvent, tissue or swab |
| Mounting caution | Retaining-ring mounts are likely to damage the coating |
| Source | Manufacturer published series specifications |
Applications
- Polarization interferometry: where the reflected beam polarization state is part of the measurement and an overcoat would bias it in a way that cannot be calibrated out
- Polarization-maintaining fibre delivery: the final fold after the collimator, where the extinction ratio achieved by the fibre must survive to the workpiece
- Ellipsometry and reflection polarimetry: instrument folds that must not add an unknown retardance between the sample and the detector
- Ultrafast beam paths: femtosecond and picosecond steering where an overcoat would contribute dispersion the compressor was not designed for
- High-power carbon dioxide work: 10.6 µm folds at power levels that a protected film would not survive, up to the 1000 W/cm continuous rating
- Fixed internal folds in sealed heads: positions that are aligned once at build and never touched again, which is exactly the environment this coating tolerates
Selection Guide
The M03 is chosen by requirement rather than by preference. Work down this list and stop at the first line that matches; if none of them matches, protected gold is probably the better buy.
| If the requirement is | Choose | Because |
|---|---|---|
| Polarization state must arrive unchanged | PF10-03-M03 | No overcoat, so no unquantifiable polarization change |
| Highest reflectance between 800 nm and 2 µm | PF10-03-M03 | 97 percent against 96 percent for protected gold |
| Highest continuous power at 10.6 µm | PF10-03-M03 | 1000 W/cm, with no overcoat absorption |
| The surface will be touched or cleaned | PF10-03-M01 | Protected gold tolerates a gentle solvent wipe |
| Visible light below 800 nm is involved | PF10-03-P01 or PF10-03-G01 | Gold reflects poorly below 800 nm |
| Working band is 2 µm and above only | PF10-03-M02 | 98 percent average and 95 percent absolute in the mid infrared |
Series Comparison
Bare gold is offered across the round sizes and in square format, all with the same 97 percent specification and the same handling rules. The damage threshold is a property of the coating, so it does not change with diameter.
| Item | Format | Diameter or face | Thickness | Clear aperture |
|---|---|---|---|---|
| PF05-03-M03 | Round | Ø12.7 mm | 6.0 mm | Ø11.4 mm |
| PF07-03-M03 | Round | Ø19.0 mm | 6.0 mm | Ø17.1 mm |
| PF10-03-M03 | Round | Ø25.4 mm | 6.0 mm | Ø22.9 mm |
| PF20-03-M03 | Round | Ø50.8 mm | 12.0 mm | Ø45.7 mm |
| PFSQ10-03-M03 | Square | 25.4 x 25.4 mm | 6.0 mm | 90 percent of face |
| PF10-03-M03-10 | Round, pack of 10 | Ø25.4 mm | 6.0 mm | Ø22.9 mm |
FAQ
Q: Why can this mirror not be cleaned at all?
A: Because bare gold has no protective layer and no hardness. Any mechanical action, including a lens tissue dragged with solvent, removes gold rather than contamination, and the removal is permanent and visible as a change in reflectance. The manufacturer permits one method only: blowing off loose dust with clean dry air or nitrogen. Solvent, tissue, swabs and drag wipes are all excluded, not merely discouraged.
Q: What do I do if someone touches the coated face?
A: Nothing, and that is the honest answer. A fingerprint leaves oil that bonds to the gold and changes the local reflectance; there is no approved method to remove it. Assess the optic where it matters, in the beam, and if the power or the wavefront has moved, replace it. Trying to rescue it will make the damage larger and more predictable in the wrong direction.
Q: Does bare gold tarnish or oxidise in air?
A: No. Gold does not oxidise at room temperature, which is why an unprotected film can survive years in a sealed head. What destroys it is contact: fingerprints, aerosols, abrasive particles, and retaining rings that scrape the surface as they are tightened. Chemical inertness and mechanical fragility coexist in the same part.
Q: Why is there a 10.6 µm pulsed rating but nothing at 1 µm?
A: The published rating of 4 J/cm² is measured at 10.6 µm with 100 ns pulses at 1 Hz. No pulsed rating is published at 1.064 µm for this coating, so there is no number to design to. If your application is a 1 µm pulsed laser, use protected gold, which is specified at 2 J/cm² at 1.064 µm.
Q: Can I hold it with a retaining ring?
A: The manufacturer warns specifically that mounts using retaining rings are likely to damage the surface of an unprotected mirror. Use a mount that holds the optic by its edge or by a clearance-fit seat, and if a ring is unavoidable, use a plastic-tipped one and bring it up only until the disc stops moving.
Q: Is it suitable for ultrafast pulses?
A: That is one of its intended uses: with no overcoat there is no added dispersion, so a pulse reflected from this surface is not stretched by the coating. The substrate still contributes material dispersion through the 6 mm of fused silica, so a double-pass fold is not dispersion free, only dispersion that you can calculate.
Usage Precautions
These five rules are the whole of the handling specification. They are quoted from the manufacturer and they are not negotiable, because every one of them describes a way to destroy the optic permanently.
- Handle by the edge, always. Latex gloves or finger cots, no exceptions. Oil from a finger reaches the gold and stays there.
- Blow only. Clean, dry air or nitrogen, from a filtered source, at a shallow angle. No solvent, no lens tissue, no cotton swab, no drag wipe, no “just this once”.
- Plan the alignment before the optic goes in. Work out the mount position, the beam height and the fold angle on paper or with a substitute blank, then fit the coated optic and leave it alone.
- Once it is in, stop touching it. No re-seating, no small adjustments by hand, no removal to check something else. Every contact is a chance to lose the part.
- Avoid retaining rings and abrasive anything. The manufacturer states that retaining-ring mounts are likely to damage an unprotected gold surface, and the same applies to tissues, foam, cardboard and bench paper.
Beyond the protocol, three practical points. Store the optic in a closed case with the coated face up and nothing resting on it; a bare gold surface will not survive a night under a lens tissue. Inspect by oblique light and by eye only, never by wiping a corner to see whether it is dirty. And dump the rear scatter: the rear face is fine ground and spreads rather than forming a clean ghost, but at 10.6 µm that spread is still heat landing somewhere.
Disclaimer
The values on this page come from the manufacturer published series tables and are provided for selection purposes only. The current official datasheet governs. Coatings, dimensions and markings may change without notice. Price and delivery are quoted separately by our sales desk.
Contact Us
If you are unsure whether your path can live with a bare gold surface, tell us how the optic will be mounted and whether anyone will ever be able to reach it. Where the answer is no, we will point you to protected gold instead of selling you a part that will not survive commissioning.








Reviews
There are no reviews yet.