Description
Thorlabs PF20-03-M03 Ø50.8 mm (2 in) Unprotected Gold Mirror, 800 nm – 20 µm
Product Overview
The PF20-03-M03 is a two-inch round mirror carrying a bare gold coating with no dielectric overcoat. The substrate is fused silica, 50.8 mm in diameter and 12.0 mm thick, polished to a surface flatness of λ/10 at 633 nm and a surface quality of 40-20 scratch-dig. The gold film delivers an average reflectance of 97 percent across the 800 nm to 20 µm band, the clear aperture is 90 percent of the diameter (45.7 mm), the front surface is intended for angles of incidence from 0° to 45°, and the part number is laser-engraved on the back side so that a mounted optic can still be identified without dismounting it.
On paper this looks like a slightly better version of the protected gold mirror next to it in the catalogue, and that reading is wrong. The protected gold part, PF20-03-M01, is specified at an average reflectance of 96 percent. The unprotected part is specified at 97 percent. One percentage point is not a purchasing argument. If reflectance were the only criterion, the M03 would never leave the shelf, because it costs more in care and attention than it returns in throughput.
The reason the M03 exists is the layer that the M01 has and the M03 does not. The overcoat that protects a gold film is a dielectric stack, and a dielectric stack is not electrically neutral to the light passing through it. Thorlabs states the consequence plainly: the overcoat of the protected mirrors results in polarization changes that can be difficult to quantify and sometimes induces absorption in the mid- to far-IR. Unprotected mirrors are therefore the recommended choice where the polarization state has to be strictly maintained, or where dispersion inside the overcoat of a protected mirror has to be avoided altogether. Read that sentence twice, because it describes two different failure modes, not one. The first is a polarization error that you cannot calibrate out, since you do not know its magnitude. The second is a wavelength-dependent phase that accumulates every time the beam bounces.
The price of that purity is mechanical. Thorlabs describes the trade-off in one line: unprotected gold offers higher reflectance than protected gold but is more delicate. Gold itself is chemically inert and does not tarnish in air, so the risk is not oxidation. The risk is contact. A fingerprint leaves an organic film that is far more absorbing than gold. An aerosol droplet leaves a dried residue with a different refractive index. An abrasive particle dragged across the surface removes metal rather than deforming it. Any of the three converts a 97 percent mirror into something considerably worse, permanently, because there is no coating to sacrifice in place of the gold.
Key Features
- Polarization state preserved through the reflection. With no dielectric overcoat in the beam path, the only interaction is with the metal itself. There is no film-induced retardance to characterise, no elliptical contamination of a linear input, and no need to build a per-mirror polarization calibration into an interferometer or a polarimeter. This is the first reason to specify the M03, and for most users it is the only reason.
- No overcoat dispersion, which matters in ultrafast work. A protected mirror adds a thin dielectric layer whose group delay dispersion varies across the pulse spectrum. In a chirped-pulse system, every folding mirror contributes a small, wavelength-dependent phase error that has to be absorbed into the compressor design. Removing the overcoat removes that term entirely, so the dispersion budget belongs to the grating pair or the prism pair alone.
- Average reflectance of 97 percent from 800 nm to 20 µm. One coating covers the near infrared, the short-wave infrared, the mid infrared and the long-wave infrared. A single part number therefore serves a Ti:sapphire beam at 800 nm and a CO₂ beam at 10.6 µm, which simplifies spares holding in a laboratory that runs more than one laser.
- Pulse damage threshold of 4 J/cm² at 10.6 µm. Measured with 100 ns pulses at 1 Hz over a 0.435 mm spot. Among the metallic coatings offered on this substrate this is the highest pulsed figure, and it reflects the fact that there is no dielectric layer to be ablated ahead of the metal.
- CW damage threshold of 1000 W/cm at 10.6 µm. Measured over a 1.18 mm spot. Again the highest of the metal films in this family, for the same structural reason: the absorbing interface between metal and overcoat, which is where CW damage usually nucleates, does not exist here.
- Fused silica substrate, λ/10 at 633 nm, 40-20 scratch-dig. The low thermal expansion of fused silica (0.55 × 10⁻⁶/°C) keeps the figure stable when the optic warms under load, and the λ/10 surface figure keeps the reflected wavefront clean enough for interferometric use rather than mere beam steering.
- 45.7 mm clear aperture on a 50.8 mm body. The 90 percent clear aperture leaves a 2.5 mm rim for the mount to grip. On an expanded beam this is the difference between using the full output and masking the edges, and it is the practical reason to move up to the two-inch size rather than stay at one inch.
Technical Specifications
| Parameter | Specification |
|---|---|
| Part Number | PF20-03-M03 |
| Coating Type | Unprotected gold (bare gold, no dielectric overcoat) |
| Spectral Range | 800 nm to 20 µm |
| Average Reflectance (Ravg) | 97% from 800 nm to 20 µm |
| Diameter | 50.8 mm (2 in), tolerance +0.0 / -0.1 mm |
| Thickness | 12.0 mm (0.47 in), tolerance ±0.2 mm |
| Substrate Material | Fused silica |
| Coefficient of Thermal Expansion | 0.55 × 10⁻⁶/°C |
| Surface Flatness | λ/10 at 633 nm (peak to valley) |
| Surface Quality | 40-20 scratch-dig |
| Clear Aperture | 90% of diameter (45.7 mm) |
| Angle of Incidence | 0° to 45° |
| Back Surface | Fine ground, part number laser-engraved |
| Pulsed Damage Threshold | 4 J/cm² at 10.6 µm, 100 ns, 1 Hz, Ø0.435 mm |
| CW Damage Threshold | 1000 W/cm at 10.6 µm, Ø1.18 mm |
| Cleanability | Not cleanable; dust removal by clean dry air or nitrogen only |
| Polarization Behaviour | No overcoat-induced polarization change; suited to strict polarization maintenance |
| Typical Mounting | Two-inch optic mount or kinematic mount with retaining ring |
The two damage thresholds above are measured values for this coating. Thorlabs notes that the threshold of a given coating does not change with the diameter of the optic, because the coating process and the coating itself are the same; what changes with diameter is how much energy the part has to survive. The measurements are made on clean optics. Surface contamination lowers the threshold substantially, which is the single most important thing to remember about a bare gold surface.
Applications
The M03 is specified by what it does not do to the beam rather than by what it does to it. The following are the situations where that distinction decides the part number.
- Polarization-maintaining beam routing. In an interferometer where the reference and measurement arms carry orthogonal linear states, every fold is a chance for the two states to pick up unequal phase. A mirror with an overcoat of unknown retardance turns that into an unquantified measurement error. A bare gold fold contributes the Fresnel phase of a metal and nothing else.
- Ellipsometry and polarimetry. Instruments that measure the polarization change caused by a sample cannot afford a component that changes polarization itself. Using the M03 on the delivery and collection folds keeps the measured ellipsometric parameters attributable to the sample.
- Quantum optics with polarization encoding. Where a qubit is encoded in the polarization of a photon, an overcoat that introduces a small, wavelength-dependent, angle-dependent transformation is a coherent error inside the interferometer. Bare gold removes a whole class of systematic error from the budget.
- Pump-probe experiments with polarization gating. When the signal is selected by the relative polarization of pump and probe, the probe path must not rotate. A chain of protected folds can accumulate enough retardance to leak pump light into the detection channel; a chain of bare gold folds cannot.
- Chirped-pulse amplification, on the dispersion budget. In a system where the compressor is tuned to cancel the stretcher to within a few hundred fs², the small dispersion of a protected fold is not negligible once there are eight or twelve of them. Removing the overcoat makes the compressor setting independent of how many folds were added.
- Mid-infrared and far-infrared beam delivery. Overcoat absorption in the mid to far infrared is the second failure mode named by Thorlabs. At 10.6 µm and beyond, a bare gold surface reflects without the thin-film absorption that a dielectric layer can introduce.
- Multi-wavelength benches. A laboratory running a Ti:sapphire oscillator at 800 nm and a CO₂ laser at 10.6 µm can hold one spare part instead of two, because the same 97 percent coating serves both ends of a very wide band.
Selection Guide
The round geometry in this family is offered in three diameters only: Ø1/2 in (12.7 mm), Ø1 in (25.4 mm) and Ø2 in (50.8 mm). There is no Ø7 mm version, and there is no intermediate 30 mm or 40 mm size; if a drawing calls for one of those, the answer is either the one-inch part with a reducing mount or the two-inch part with an aperture mask, not a special order. The two-inch part on this page is the largest of the three and the only one with a 12.0 mm body; the two smaller sizes are 6.0 mm thick.
Size the optic from the beam, not from the mount. The clear aperture is 90 percent of the diameter, so a two-inch mirror gives 45.7 mm of usable surface. A beam that is clipped at the edge of a fold does not merely lose power; it acquires a diffraction fringe that propagates into the far field and shows up as structure in a focus. Sizing the clear aperture at 1.5 to 2 times the 1/e² beam diameter keeps the beam clear of the rim at the 45° end of the specified incidence range, where the footprint on the surface stretches by a factor of about 1.41 in one axis.
Choose between the gold variants by asking what the coating must not do. If the answer is “must not change polarization” or “must not add dispersion”, the M03 is the correct part and the M01 is the wrong one, regardless of the one-point reflectance difference. If the answer is “must survive handling, cleaning and a shared laboratory”, the M01 is the correct part and the M03 will not last. If the wavelength sits below 800 nm, neither gold part works and the choice moves to the protected silver P01 for the visible and near infrared, or the UV enhanced aluminium F01 below 450 nm. If the application is a CO₂ line at 10.6 µm and maximum reflectance at that single line matters more than broadband behaviour, the L01 line-optimised gold is the better fit.
Mounting follows from the thickness. A 12.0 mm body in a two-inch mount is stiff enough that a retaining ring tightened by hand is sufficient; there is no need to torque it, and doing so prints the ring’s shape into the λ/10 surface. For kinematic use, a two-inch kinematic mount with three adjusters and a nylon-tipped retaining ring holds the figure without marking the ground edge.
Series Comparison
The PF20-03 body is available with seven metallic coatings. They differ in spectral range, in average reflectance and, decisively for this page, in whether a dielectric overcoat is present.
| Code | Coating | Spectral Range | Average Reflectance | Overcoat |
|---|---|---|---|---|
| F01 | UV enhanced aluminium | 250-450 nm | Ravg 90% | Protected |
| G01 | Protected aluminium | 450 nm-20 µm | Ravg 90% (450 nm-2 µm), 95% (2-20 µm) | Protected |
| P01 | Protected silver | 450 nm-20 µm | Ravg 97% (450 nm-2 µm), 95% (2-20 µm) | Protected |
| M01 | Protected gold | 800 nm-20 µm | Ravg 96% | Protected |
| M02 | MIR enhanced gold | 2-20 µm | Ravg 98% | Protected |
| M03 | Unprotected gold | 800 nm-20 µm | Ravg 97% | None |
| L01 | Unprotected gold, line optimised | 10.6 µm line | Ravg 99% | None |
Read the last column as the design intent. Everything marked protected is built to be handled, cleaned and shared. Everything marked none is built to be installed once and left alone. The M03 is the broadband member of the unprotected group, covering 800 nm to 20 µm at 97 percent, while the L01 gives up bandwidth to reach 99 percent at the 10.6 µm CO₂ line. Between the two gold parts with overcoats, the M01 covers the same 800 nm to 20 µm band at 96 percent and the M02 trades bandwidth for 98 percent in the 2-20 µm window.
FAQ
Q1. For a polarization-sensitive setup, is the M03 actually worth the difference over the M01?
Yes, if polarization is a specification rather than a convenience. The M01 reflects 96 percent and the M03 reflects 97 percent, and no project has ever been saved by that point. What the M03 buys is the absence of a dielectric overcoat in the beam path. Thorlabs notes that the overcoat of protected mirrors produces polarization changes that are difficult to quantify. Difficult to quantify is the operative phrase: an error you can measure can be compensated, an error you cannot quantify becomes an uncertainty term that sits in your error budget forever. If your specification says the polarization extinction ratio must be maintained through the fold, the M03 is the part that lets you claim it.
Q2. What does “unprotected” cost me in day-to-day laboratory practice?
It costs you the right to clean the optic. There is no sacrificial layer, so any mechanical action removes gold. In practice this means the mirror is installed once, aligned with the beam blocked or heavily attenuated, and thereafter left alone. Dust is removed with clean dry air or dry nitrogen only. If a fingerprint lands on the surface, the optic is degraded and there is no recovery procedure, because every procedure that would remove the fingerprint would also remove metal.
Q3. Can the surface be cleaned with acetone or methanol if something lands on it?
No. Solvent cleaning is appropriate for protected coatings, where the overcoat takes the mechanical action of the tissue and the metal underneath is never touched. On a bare gold surface the solvent does not dissolve the gold, but the wiping motion does remove it, and a solvent that leaves a drying mark leaves a permanent scattering site. For the M03 the accepted procedure is blow-off with clean dry air or nitrogen. No solvent, no lens tissue, no drag.
Q4. Why is the surface figure quoted at 633 nm when my laser runs at 800 nm or 10.6 µm?
Because 633 nm is the helium-neon line on which the interferometric test is performed, and a figure quoted at a test wavelength is a statement about the physical shape of the surface, not about the phase at your wavelength. A λ/10 peak-to-valley deviation at 633 nm corresponds to about 63 nm of physical sag. That same 63 nm of sag produces a much smaller fraction of a wave at 10.6 µm, so the mirror is optically flatter at your wavelength than the specification suggests, not worse.
Q5. The pulsed threshold is quoted at 10.6 µm with 100 ns pulses. Can I scale it to 1064 nm with 10 ns pulses?
Not by arithmetic. Damage thresholds depend on wavelength through the absorption of the film, on pulse duration through the heat diffusion time, and on spot size through the area over which defects are sampled. Thorlabs publishes a measured figure for a stated set of conditions; it is a comparison value between coatings, not a universal limit. For a 1064 nm nanosecond application, treat 4 J/cm² as an indication that this is a high-threshold metal film and then verify experimentally at your own fluence, starting well below and increasing in steps.
Q6. Does the 90 percent clear aperture mean I lose the outer 5 mm of the mirror?
It means the outer 5 mm is not guaranteed to meet the surface figure and surface quality specifications. Mechanically the substrate is 50.8 mm across, and the ground edge is part of the mounting surface. Optically, the specified 45.7 mm is what you may use. A beam that fills the full 50.8 mm will be partly clipped by the mount’s retaining ring in any case, so plan the beam to stay inside 45.7 mm.
Usage Precautions
- No solvent, no tissue, no drag. The only accepted cleaning action on a bare gold surface is blow-off with clean dry air or dry nitrogen. There is no wet cleaning procedure, no first-aid wipe, and no “gentle” version of one. If the surface is contaminated, the optic is replaced, not restored.
- Handle by the ground edge only, with gloves. Nitrile or latex gloves, and fingers on the 2.5 mm rim, never on the coated face. A fingerprint on bare gold is an absorbing organic film that no subsequent step will remove.
- Align with the beam attenuated or blocked. The moment of highest risk is the moment of installation, when hands, tools and the mount are all near the coated face. Bring the beam up after the optic is clamped and the tools are away.
- Do not over-clamp the retaining ring. A 12.0 mm fused silica body is stiff, but a ring tightened with a tool will still print a ring-shaped figure error into a λ/10 surface. Hand-tight is enough, and nylon-tipped rings are preferable.
- Keep the part in its original case until installation. The supplied case holds the optic off its faces. Do not stack bare gold mirrors, do not wrap them in paper, and do not store them in a drawer with loose hardware, because a single abrasive particle in contact with the surface under the weight of the optic is enough to scratch it.
- Respect the cleanliness assumption behind the damage thresholds. The published 4 J/cm² and 1000 W/cm are measured on clean optics. Dust, fingerprints and outgassed films lower the threshold substantially, and on a bare gold surface those contaminants cannot be removed, so the effective threshold of a contaminated part is unknown and lower than the specification.
- Store dry, but not for the reason you would store a silver mirror. Gold does not oxidise, so humidity is not a chemical threat. It is a contamination vector, because condensation concentrates airborne material on the surface. A desiccated cabinet is still the right home for the part.
Disclaimer
The specifications on this page are compiled from Thorlabs’ publicly published product documentation and are provided for selection reference only. In case of any discrepancy, the current official datasheet from the manufacturer prevails. Product specifications, coatings and appearance are subject to change without prior notice. Damage thresholds are measured values under the stated test conditions and are not a guarantee of performance in any particular setup; users are responsible for verifying suitability at their own fluence, wavelength, pulse duration and beam size. Prices and lead times are confirmed by our sales team at the time of quotation and are not implied by this page.
Contact Us
For technical selection support, a quotation, or help deciding between the unprotected and protected gold variants for your optical layout, please contact our sales team.
Hotline: +86 159-2722-0467
E-mail: 859818709@qq.com | Website: www.soar-laser.cn
We support single-unit purchases for laboratory evaluation as well as volume orders, and we can advise on mounting hardware, spare-part strategy and lead time for the two-inch mirror family.








Reviews