Description
This is the 10-piece pack of the PF10-03-G01; the optic is identical to the single-unit version.
Product Overview
Ten Ø25.4 mm fused silica mirrors, 6.0 mm thick, with protected aluminium: a silicon dioxide overcoat on an aluminium film, specified at 90 percent average reflectance from 450 nm to 2 µm and 95 percent from 2 to 20 µm. Figure is λ/10 at 633 nm, surface 40-20 scratch-dig, parallelism 3 arcmin, clear aperture 90 percent of the diameter, and each rear face is fine ground and laser engraved with the item number.
The reason to keep ten of these on the shelf is breadth. No other single metal film in this catalogue spans the visible, the near infrared and the mid infrared in one part: 532 nm, 633 nm, 808 nm, 1064 nm and 10.6 µm are all inside the specified range. A workshop where jobs of different wavelengths share the same benches normally needs three or four different mirror types, three or four bins, and a standing risk of fitting the wrong one. One part number removes that risk, and ten of them remove it for every station at once.
Aluminium is also the most forgiving film to live with. It is the closest match to bare aluminium reflectance of any protected coating, which is what makes it the general-purpose choice, and the silica overcoat makes the surface wipeable and gives it a much smaller chance of tarnishing than protected silver in humid air. That combination is what a production environment actually needs: an optic that can be cleaned when it gets dirty, in a shop that is not a cleanroom, without the film going milky after a season.
What aluminium is not good at is high average power in the near infrared. Aluminium absorbs around 1 µm far more than silver does, which is why the published CW rating for this coating at 1.070 µm is an order of magnitude below the silver figure. For a low-power fold, an alignment path or a 10.6 µm beam the part is excellent; for a multi-hundred-watt 1064 nm delivery path, the protected silver pack is the correct choice and this one is not.
Key Features
- Ten optics, one part number: the same coating and figure as the single unit, from the same production runs
- 450 nm to 20 µm in one film: visible, near infrared and mid infrared from a single spare, so mixed-wavelength shops stop stocking several mirror types
- Silicon dioxide overcoat: wipeable, and far slower to tarnish than protected silver in humid air
- Closest to bare aluminium reflectance: the general-purpose metal coating, with no colour cast and no narrow band to respect
- λ/10 figure, 40-20 surface, 3 arcmin parallelism: full single-unit specification in every optic in the pack
- 0.3 J/cm² at 1064 nm and 350 W/cm CW at 10.6 µm: enough for marking, engraving and most industrial folds, not enough for high-power 1 µm delivery
- Laser engraved rear faces: identification survives installation in a closed head
Technical Specifications
| Model | PF10-03-G01-10 |
| Pack size | 10 mirrors, each identical to the PF10-03-G01 |
| Coating | Protected aluminium |
| Overcoat | Silicon dioxide (SiO2) |
| Wavelength range | 450 nm – 20 µm |
| Average reflectance | Ravg 90% from 450 nm to 2 µm; Ravg 95% from 2 to 20 µm |
| Substrate | Fused silica |
| Diameter | Ø25.4 mm (1 in) per optic |
| Diameter tolerance | +0.0 mm / -0.1 mm |
| Thickness | 6.0 mm (0.24 in) |
| Thickness tolerance | ±0.2 mm |
| Surface flatness | λ/10 at 633 nm |
| Surface quality | 40-20 scratch-dig |
| Parallelism | 3 arcmin or better |
| Clear aperture | 90 percent of the diameter |
| Damage threshold, pulsed | 0.3 J/cm² at 1064 nm (10 ns, 10 Hz, Ø1.000 mm) |
| Damage threshold, CW | 100 W/cm at 1.070 µm (Ø0.098 mm); 350 W/cm at 10.6 µm (Ø0.339 mm) |
| Rear surface | Fine ground, engraved with the item number |
| Source | Thorlabs official series specification table |
Applications
- Mixed-wavelength workshop folds: one spare part covers visible alignment lasers, 1064 nm marking heads and 10.6 µm engravers on the same floor
- Carbon dioxide laser gantries: 10.6 µm sits well inside the band and the CW rating at that wavelength is the highest of any band this coating covers
- Fibre laser marking and engraving heads: beam delivery folds at moderate power, where aluminium durability matters more than the last few percent of reflectance
- Machine vision and illumination folds: white light and near infrared illumination paths, where a neutral film avoids colour shift
- Alignment and commissioning targets: a mirror that can be wiped, swapped and re-wiped without ceremony during a build
Selection Guide
| Working band | Coating to order | Average reflectance | Note |
|---|---|---|---|
| 250 – 450 nm | UV-enhanced aluminium, -F01 | 90% | The only option below 450 nm |
| 450 nm – 20 µm | Protected aluminium, -G01 (this page) | 90% to 2 µm; 95% beyond | Widest single-film coverage, most durable to cleaning |
| 450 nm – 20 µm, highest visible reflectance | Protected silver, -P01 | 97% to 2 µm; 95% beyond | Brighter, but tarnishes faster and is less tolerant of wiping |
| 800 nm – 20 µm | Protected gold, -M01 | 96% | Flat infrared response, softer surface |
| 2 – 20 µm | MIR-enhanced gold, -M02 | 98% | Best mid-infrared reflectance |
Series Comparison
| Pack item | Coating | Band | Average reflectance | Damage threshold, pulsed |
|---|---|---|---|---|
| PF10-03-G01-10 | Protected aluminium | 450 nm – 20 µm | 90% to 2 µm; 95% beyond | 0.3 J/cm² at 1064 nm |
| PF10-03-P01-10 | Protected silver | 450 nm – 20 µm | 97% to 2 µm; 95% beyond | 1 J/cm² at 1064 nm |
| PF10-03-M01-10 | Protected gold | 800 nm – 20 µm | 96% | 2 J/cm² at 1064 nm |
| PF10-03-F01-10 | UV-enhanced aluminium | 250 – 450 nm | 90% | 0.3 J/cm² at 355 nm |
| PF05-03-G01-10 | Protected aluminium | 450 nm – 20 µm | 90% to 2 µm; 95% beyond | 0.3 J/cm² at 1064 nm |
FAQ
Q: Protected aluminium or protected silver?
A: Silver is brighter in the visible and near infrared and has the higher damage threshold; aluminium covers the same band, costs less, and survives humidity and repeated cleaning better. Choose silver when the power budget or the pulse energy demands it, aluminium when the environment is the problem.
Q: Can I wipe this mirror?
A: Yes, that is one of its advantages over gold, but wipe rarely and gently: blow off loose dust first, then lens tissue with solvent, one direction, no pressure. The silica overcoat is thin, and a habit of daily wiping will wear through it in the same way it wears through any protected film.
Q: How much pulse energy does 0.3 J/cm² allow?
A: Over the Ø1.000 mm test spot the rated fluence corresponds to roughly 2.4 mJ per pulse at 1064 nm with 10 ns pulses. That covers marking and trimming duties and rules out most kilowatt-class delivery paths. If your pulse energy is within a factor of two of that number, move to the protected silver pack rather than running this coating at its limit.
Q: Why is the CW rating so much lower than the silver rating at 1 µm?
A: Because aluminium absorbs more than silver at that wavelength, so the same beam deposits more heat in the film. The published figure of 100 W/cm at 1.070 µm is not a typo next to the 500 W/cm for silver; it is the physics of the metal. At 10.6 µm the gap closes and aluminium reaches 350 W/cm.
Q: Does the pack help with traceability?
A: Partly. All ten carry the same engraved item number, so the engraving tells you what the optic is, not which one it is. Pair it with a station log: position, install date, hours, reason for replacement.
Q: Is there a downside to standardising on one coating?
A: Only where the wavelength or the power demands something else. Standardising on protected aluminium is right for a shop running visible and mid-infrared work at moderate power; it is wrong for a high-average-power 1064 nm line, where the reflectance and the damage threshold both favour silver.
Usage Precautions
- Stay inside the fluence rating. Aluminium at 1 µm is the weakest point of this coating, and the failure mode is a small pit that grows with every subsequent pulse.
- Do not stack the optics face to face in storage; ten coated surfaces in one box will scratch each other. Keep them separated.
- Block rear reflections. The rear face is fine ground, so it scatters rather than forming a clean ghost, but that scatter still has to go somewhere other than a detector or an operator.
- Keep the film dry between jobs. Condensation on a cold optic pulled out of a warm humid room is the usual route to a milky surface.
- Check the part before fitting it. UV-enhanced and protected aluminium look almost identical in a mount, and fitting the wrong one shows up as a power shortfall that looks like a laser fault.
Disclaimer
Specifications on this page are compiled from the manufacturer’s published series tables and are provided for selection purposes only. The current official datasheet governs. Dimensions, coatings and markings may change without notice. Price and delivery are quoted separately by our sales desk.
Contact Us
Questions about fit, coating choice or lead time go to our technical desk. Send the part number, the wavelength, the beam diameter at the optic and the intended incidence angle, and you will get an answer that names a specific part rather than a range of options. Bulk and project quantities are quoted individually.









Reviews