QQ: 859818709

Thorlabs PF20-03-P01 Ø50.8 mm (2 in) Protected Silver Mirror, 450 nm – 20 µm

Thorlabs PF20-03-P01 Ø50.8 mm (2 in) Protected Silver Mirror, 450 nm – 20 µm

Price on request
Category:

Description

Thorlabs PF20-03-P01 Ø50.8 mm (2 in) Protected Silver Mirror, 450 nm – 20 µm

Product Overview

The strongest metal film in the visible and near infrared

The PF20-03-P01 is a two-inch round mirror with a silver coating protected by a silicon dioxide layer about 100 nm thick. Its average reflectance is 97 percent from 450 nm to 2 µm and 95 percent from 2 to 20 µm. The substrate is fused silica, 50.8 mm in diameter and 12.0 mm thick, polished to λ/10 at 633 nm with a 40-20 scratch-dig surface quality and a clear aperture of 90 percent of the diameter (45.7 mm). The part number is laser-engraved on the fine-ground rear face.

Across the visible and into the near infrared, silver is the highest-reflectance metallic coating available, and Thorlabs states the position without qualification: in the visible to near-infrared spectral range, silver mirrors are the highest-reflectance metallic mirrors, and they also offer high reflectance in the infrared. There is no aluminium or gold coating that beats silver between 450 nm and 2 µm. This is why the coating exists and why it is the default choice for a visible ultrafast beamline, a Ti:sapphire system or a multi-wavelength illumination path.

Why a 100 nm overcoat is not a detail

Silver is also the only precious metal used in mirror coatings that is chemically attacked in ordinary laboratory air. Sulphur compounds tarnish it to silver sulphide, which is brown and absorbing; humidity accelerates the reaction; fingerprints leave chloride and organic residues that attack the film locally. A bare silver mirror therefore degrades in weeks in a normal room, which is why the coating is always overcoated.

The overcoat is silicon dioxide, roughly 100 nm thick. It is thin enough that the optical penalty is small and thick enough to be a continuous barrier. But it is not zero: the measured 97 percent average from 450 nm to 2 µm is the reflectance of the finished, overcoated part, not the reflectance of bare silver, and the difference between the two is what the protective layer costs. A hundred nanometres is also thin enough that a scratch which penetrates it exposes silver directly, which is why the handling rules for this optic are stricter than for a protected aluminium mirror.

The environment is part of the specification

Thorlabs is explicit about the limit: although the protective layer prevents the silver from oxidising, the mirror must not be used in a high-humidity environment. This is not a caution about cosmetics. A silica layer of this thickness is a diffusion barrier, not a hermetic seal, and water vapour that reaches the silver through pinholes or through the layer itself starts the sulphidation reaction from underneath, where it cannot be seen until the reflectance has already fallen. A silver mirror in a humid enclosure fails from the back of the coating forward, and by the time the front looks dull the damage is old.

The practical consequence is that the P01 belongs in a temperature-controlled, low-humidity laboratory, and it should be stored in a desiccated cabinet when it is not mounted. A mirror used at ambient humidity in a tropical or coastal site will have a shorter service life than the same part used in a dry inland laboratory, and no amount of care at the bench changes that.

Key Features

  1. Highest metallic reflectance from the visible into the near infrared. 97 percent average from 450 nm to 2 µm. Against the protected aluminium coating at 90 percent over the same window, the silver recovers seven percentage points per reflection; over a six-fold path the silver throughput works out at about 83 percent against about 53 percent for aluminium, a difference of thirty percentage points. This is the number that decides most visible-wavelength layouts.
  2. Still strong in the infrared at 95 percent from 2 to 20 µm. Silver does not fall off a cliff at 2 µm; it drops from 97 to 95 and stays there out to 20 µm, which means one coating covers a Ti:sapphire fundamental, its harmonics, a near-infrared OPA and a mid-infrared idler without changing part numbers.
  3. Silicon dioxide overcoat, about 100 nm thick. The layer is what makes the coating usable at all: it prevents the silver from oxidising and it is thick enough to take the incidental contact that a mounted optic receives during alignment. It is also thin enough that the optical cost is confined to the reflectance figure already quoted.
  4. Four published laser damage thresholds. 0.225 J/cm² at 800 nm with 99 fs pulses at 1 kHz over a 0.167 mm spot; 1 J/cm² at 1064 nm with 10 ns pulses at 10 Hz over a 1.010 mm spot; 500 W/cm CW at 1.07 µm over a 0.974 mm spot; 1500 W/cm CW at 10.6 µm over a 0.339 mm spot. Four conditions, four numbers, no interpolation required.
  5. λ/10 at 633 nm surface figure. Tight enough for interferometric and wavefront-sensitive use, not merely for beam steering. The test is performed at the helium-neon line, so the figure is a statement about the physical shape of the surface.
  6. 40-20 scratch-dig surface quality on a 12.0 mm fused silica body. The thick body resists the print-through that a thin substrate shows when a retaining ring is tightened, and fused silica’s 0.55 × 10⁻⁶/°C expansion keeps the figure stable as the optic warms.
  7. 45.7 mm clear aperture with an engraved part number on the back. Enough usable aperture for an expanded beam, and identification that survives years in a mount.

Technical Specifications

Parameter Specification
Part Number PF20-03-P01
Coating Protected silver, silicon dioxide overcoat approximately 100 nm thick
Spectral Range 450 nm to 20 µm
Average Reflectance, 450 nm to 2 µm 97%
Average Reflectance, 2 to 20 µm 95%
Diameter 50.8 mm (2 in), +0.0 / -0.1 mm
Thickness 12.0 mm (0.47 in), ±0.2 mm
Substrate Fused silica, CTE 0.55 × 10⁻⁶/°C
Surface Flatness λ/10 at 633 nm, peak to valley
Surface Quality 40-20 scratch-dig
Clear Aperture 90% of diameter (45.7 mm)
Angle of Incidence 0° to 45°
Rear Surface Fine ground, part number laser-engraved
Pulsed Damage Threshold, Femtosecond 0.225 J/cm² at 800 nm, 99 fs, 1 kHz, Ø0.167 mm
Pulsed Damage Threshold, Nanosecond 1 J/cm² at 1064 nm, 10 ns, 10 Hz, Ø1.010 mm
CW Damage Threshold, 1.07 µm 500 W/cm at 1.07 µm, Ø0.974 mm
CW Damage Threshold, 10.6 µm 1500 W/cm at 10.6 µm, Ø0.339 mm
Environmental Limit Must not be used in a high-humidity environment
Recommended Handling Latex or nitrile gloves; do not touch the coated face or the edge

Read the four damage figures as four different tests, not as one number quoted four ways. The 0.225 J/cm² figure comes from 99 fs pulses, where the damage mechanism is multiphoton absorption and the threshold is dominated by the electric field; the 1 J/cm² figure comes from 10 ns pulses, where heat diffusion during the pulse matters and the threshold is higher in fluence but lower in peak power. The two CW figures differ by a factor of three because both the wavelength and the spot size differ: 500 W/cm at 1.07 µm over a 0.974 mm spot and 1500 W/cm at 10.6 µm over a 0.339 mm spot. Do not carry a number from one row to another application.

Applications

The P01 is chosen for one reason: the wavelength is in the window where silver is the best metal available. Everything below follows from that.

  • Ti:sapphire oscillators and amplifiers. The 800 nm centre wavelength sits in the middle of the 97 percent window. A regenerative amplifier with eight intra-cavity or intra-chain folds delivers about 78 percent of the circulating power with silver coatings and about 43 percent with aluminium, which is usually the difference between needing a second amplifier stage and not needing one.
  • Visible and near-infrared ultrafast beamlines. White-light continua seeded from a sapphire plate, non-collinear optical parametric amplifiers and their pump arms all need broadband high reflectance from 500 nm to 900 nm. Silver is the only metal that delivers it.
  • Harmonic generation. Second and third harmonic outputs at 400 nm and 267 nm are outside the silver window’s short end, so those folds need a different coating; but the residual fundamental that has to be separated and dumped can be routed with the P01, which keeps the high-power path on the highest-reflectance metal.
  • Multi-wavelength illumination and imaging. Where a broadband source from 450 nm to 2 µm is folded several times, the seven-point advantage over aluminium compounds with each reflection, and the colour balance of the delivered light is preserved because the reflectance is flat across the window rather than sloped.
  • Spectroscopy and detection benches. A flat, high reflectance across the visible reduces the wavelength-dependent calibration that a lower-reflectance coating forces on a spectrometer’s collection optics.
  • Femtosecond micromachining at 800 nm. With 99 fs pulses the 0.225 J/cm² threshold is the governing number; a 100 fs pulse train at 1 kHz with a 0.167 mm spot reaches that fluence at about 49 µJ per pulse, which sets the upper bound for the fold in a micromachining delivery path.

Selection Guide

Start from the wavelength, because that is what decides the metal. Then check the environment, because that is what decides whether silver is allowed at all.

  • 450 nm to 2 µm. Silver, 97 percent. This is the widest high-reflectance window of any metal coating in the family and the default answer for visible and near-infrared work.
  • 250 nm to 450 nm. UV enhanced aluminium, 90 percent. Silver is not usable here; its reflectance collapses in the blue and near ultraviolet.
  • 2 µm to 20 µm, broadband. Protected gold at 96 percent or unprotected gold at 97 percent, depending on whether the coating must be cleanable. Silver’s 95 percent is respectable but no longer the best.
  • 2 µm to 20 µm, maximum reflectance. Mid-infrared enhanced gold at 98 percent, which trades the visible and near-infrared bands for the best figure above 2 µm.
  • 10.6 µm single line. Line-optimised unprotected gold at 99 percent, if the only wavelength that matters is the CO₂ line.
  • Any of the above in a humid enclosure. Silver is excluded. Thorlabs states that the protective layer prevents oxidation but that the mirror must not be used in a high-humidity environment, so a humid or condensing location moves the choice to aluminium or gold regardless of the reflectance penalty.

Size from the beam. The clear aperture is 45.7 mm on this two-inch body; the round sizes in the family are Ø1/2 in (12.7 mm), Ø1 in (25.4 mm) and Ø2 in (50.8 mm), with no Ø7 mm option. A 45° fold stretches the beam footprint by about 1.41 in one axis, so a beam that is 30 mm across becomes 42 mm on the surface, which is inside the clear aperture but close enough to the rim that the mount’s retaining ring has to be checked.

Series Comparison

The cleanest way to compare the metallic coatings is by wavelength window, because that is the order in which a real selection decision is made. The table below inverts the usual presentation and leads with the window.

Wavelength Window Coating to Choose Average Reflectance Reason
250-450 nm F01, UV enhanced aluminium 90% The only metal in the family with usable ultraviolet reflectance
450 nm-2 µm P01, protected silver 97% Highest reflectance of any metallic coating in this window
450 nm-20 µm, general purpose G01, protected aluminium 90% (450 nm-2 µm), 95% (2-20 µm) The most forgiving coating where absolute reflectance is secondary
800 nm-20 µm M01, protected gold 96% Cleanable and stable, the safe choice for shared laboratories
2-20 µm, maximum reflectance M02, MIR enhanced gold 98% Best average above 2 µm, at the cost of the visible band
800 nm-20 µm, no overcoat M03, unprotected gold 97% Where overcoat dispersion or polarization change must be avoided
10.6 µm line L01, unprotected gold, line optimised 99% Maximum reflectance at a single CO₂ line, no broadband use

Notice what the table makes obvious: silver owns one row and one row only, but that row covers the entire visible and near-infrared range where most ultrafast and most imaging work happens. The 97 percent figure is seven points above aluminium and one point above gold in the same window, and unlike gold it is available all the way down to 450 nm. The cost is the row that is not in the table: there is no row for “450 nm to 2 µm in a humid enclosure”, because silver cannot go there.

FAQ

Q1. Which reflectance figure is correct: the one on this page, or the higher one quoted elsewhere?

For this product the official single-unit specification is 97 percent average from 450 nm to 2 µm and 95 percent average from 2 to 20 µm, and those are the figures used throughout this page. Some catalogue pages, multi-piece listings and third-party summaries quote a figure of ninety-seven point five percent, either by rounding or by carrying a value across from a different coating or a different product family. Where the number enters a design calculation, use the single-unit official specification: 97 percent in the visible and near infrared, 95 percent beyond 2 µm.

Q2. Can I clean a protected silver mirror with solvent?

Only with care, and only with the right materials. The protective layer is a silicon dioxide film about 100 nm thick, not a broadband dielectric mirror coating, and it can be damaged by the same actions that would damage any thin film. If cleaning is unavoidable, use reagent-grade acetone, methanol or isopropanol with lens tissue, drag once in one direction, and stop. Do not rub, do not use a dry tissue on a dry surface, and do not use any solvent that leaves a residue. Thorlabs recommends latex or similar gloves during handling, and notes that even with gloves the coated face and the edge should not be touched.

Q3. How long will the mirror last in a normal laboratory?

It depends almost entirely on humidity, not on time. Thorlabs states that although the protective layer prevents oxidation, the mirror must not be used in a high-humidity environment, and that fingerprints, contact with abrasive surfaces and high humidity or high temperature will weaken the protective layer and make the silver film prone to oxidation and degradation. In a temperature-controlled, low-humidity laboratory with the optic kept mounted and undisturbed, service life is long. In a humid or condensing location, or in a bench that is handled daily, it is not, and the reflectance will fall before anything visible appears on the surface.

Q4. What is the difference between this coating and the broadband dielectric mirrors?

Different product families entirely. The P01 is a metal film with a thin protective overcoat: broadband by nature, from 450 nm to 20 µm, with a reflectance of 97 and 95 percent and essentially no dispersion design. A broadband dielectric mirror is a multilayer stack engineered for one band, typically achieving 99 percent or more inside that band and nothing outside it, and it costs considerably more. If the requirement is “high reflectance across a wide band with one part number”, the metal film wins; if it is “maximum reflectance at one wavelength or one octave”, the dielectric wins.

Q5. Why do the two CW thresholds differ by a factor of three?

Because they are measured at different wavelengths and different spot sizes. The 500 W/cm figure is at 1.07 µm over a 0.974 mm spot; the 1500 W/cm figure is at 10.6 µm over a 0.339 mm spot. A smaller spot concentrates the same power density over a shorter thermal diffusion length, and the absorption of the film differs between the two wavelengths. Neither number can be scaled to a third wavelength by ratio; use the row that matches your laser, and if none matches, treat the closest row as an order-of-magnitude guide and test.

Q6. Does the silver coating work at 45°?

The specified angle of incidence range is 0° to 45°, so 45° is inside the specification. Be aware that the reflectance curve for a metal at 45° differs from normal incidence and differs between s and p polarization, with the p component showing the characteristic dip near the principal angle. For most beam-steering applications the difference is a few percent and is acceptable; for a polarization-critical or photometric application, characterise the fold at the working angle rather than assuming the normal-incidence figure.

Usage Precautions

Silver is the most sensitive coating in this family, and the rules that follow are not generic optics hygiene. They are the specific measures that keep a 100 nm silica layer intact over a reactive metal.

  • Control the humidity. This is the first rule and the one most often ignored. The mirror must not be used in a high-humidity environment. Keep it in a desiccated cabinet when unmounted, avoid enclosures where condensation can form, and let a cold optic come to room temperature in its sealed case before opening it.
  • Wear latex or nitrile gloves and still do not touch the surface. Thorlabs recommends gloves, and adds the important qualification: even with this protection, the coated face and the edge should not be touched. Skin oils and salts attack the silver through pinholes in the overcoat, and the edge is where the coating is thinnest.
  • Keep the optic away from sulphur, rubber and foam. Vulcanised rubber, some foams and many cardboard and paper products release sulphur compounds that tarnish silver. Do not store the mirror in contact with them, and do not leave it in a foam-lined box for years.
  • Never place it face-down. The 40-20 surface is a specification, not a guarantee against contact. A mirror set down face-first on a bench is being scratched by its own weight plus whatever particle is under it.
  • Clean rarely and gently. Reagent-grade acetone, methanol or isopropanol with lens tissue, one direction, one pass. No dry rubbing, no repeated passes over the same spot, no abrasive cloth. If a mark does not come off in one pass, it is probably under the overcoat and no further work will remove it.
  • Clamp by the rim with a nylon-tipped ring. A 12.0 mm fused silica body tolerates hand-tight clamping, but a metal ring tightened with a tool will mark the ground edge and can chip the coating at the boundary.
  • Verify before trusting a stored optic. A silver mirror that has been in storage should be checked against a known-good reference before it goes into a critical path, because the earliest stage of degradation is a small reflectance loss with no visible change.

Disclaimer

The specifications on this page are compiled from Thorlabs’ publicly published product documentation and are provided for selection reference only. Where this page and the manufacturer’s current official datasheet differ, the official datasheet prevails. Coatings, specifications and appearance may change without notice. Damage thresholds are measured values under the stated test conditions and are not a performance guarantee; the user is responsible for verifying suitability at the actual wavelength, pulse duration, repetition rate, spot size and environment. Reflectance figures are average values over the stated bands, not minimum values at every wavelength. Prices and lead times are confirmed at quotation and are not implied by this page.

Contact Us

If you need help deciding whether silver is permissible in your environment, or want a comparison against aluminium or gold for a specific wavelength, please contact us.

Hotline: +86 159-2722-0467

E-mail: 859818709@qq.com  |  Website: www.soar-laser.cn

We can supply the two-inch protected silver mirror from stock where available, advise on desiccated storage and mounting hardware, and quote the equivalent protected aluminium or gold part when humidity rules silver out.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF20-03-P01 Ø50.8 mm (2 in) Protected Silver Mirror, 450 nm – 20 µm”

Your email address will not be published. Required fields are marked *

中文EN