Thorlabs PF2011-G01 Ø50.8 mm (2 in) Zerodur® Protected Aluminum Mirror, 450 nm – 20 µm

Product Overview

A surprising number of laser benches are asked to carry two wavelengths that have nothing in common. A pump-probe experiment runs 515 nm and 10.6 µm. A materials station marks with a 1064 nm fibre laser and then inspects with a mid-infrared camera. A gas-sensing rig uses a 532 nm alignment beam to steer an invisible 4 µm probe. In each case somebody eventually asks the obvious question: is there one mirror that covers both ends, so the fold does not have to be swapped when the experiment changes?

The PF2011-G01 is that mirror, and the qualifier is important: it covers both ends and holds its figure while doing so, because the coating sits on a Zerodur® body rather than on ordinary glass. The part is a round optic 50.8 mm (2 in) in diameter and 12.0 mm (0.47 in) thick, coated with protected aluminum behind a SiO₂ overcoat, specified from 450 nm to 20 µm with an average reflectance of 90 percent from 450 nm to 2 µm and 95 percent from 2 to 20 µm. Front surface flatness is λ/10 at 632.8 nm, surface quality is 40-20 scratch-dig, the clear aperture is 45.7 mm, parallelism is 3 arcmin or better, the working range of incidence angles is 0° to 45°, and the part number is laser-engraved on the fine-ground back face.

Those two reflectance numbers cause more confusion than any other pair of figures on the datasheet, so deal with them first. They are not two measurements of the same quantity, and they do not average into a single performance figure. The first, 90 percent, is the average over the 450 nm to 2 µm interval, a span of 1.55 µm. The second, 95 percent, is the average over the 2 to 20 µm interval, a span of 18 µm, more than ten times wider. Averaging them to a single number in the low nineties would describe no wavelength at all, because each figure applies only inside its own interval and neither is a guarantee at any particular point inside it. If your work sits at 632 nm, the number that matters is whatever the coating does at 632 nm, which is not published as a single value and is best confirmed against the measured curve; the 90 percent average is a statement about the band, not about your line.

Interval Width Average Reflectance What the figure is for
450 nm – 2 µm 1.55 µm 90 percent Visible, near infrared and short-wave infrared alignment and delivery
2 – 20 µm 18 µm 95 percent Mid and far infrared, including the 10.6 µm CO₂ line

Why does the curve step up at 2 µm instead of staying flat? Aluminum is a good reflector on both sides of that boundary, but on the short side the measured reflectance is pulled down by absorption at the metal-dielectric interface, where a residual oxide or hydroxide layer survives the coating process. That interfacial absorption is a feature of the metal, not of the substrate, and it is one of the reasons the SiO₂ overcoat is deposited in the same vacuum cycle as the aluminum rather than in a second run: the less the fresh metal sees the atmosphere, the less of that interface layer forms. Above 2 µm the interface absorption is no longer significant and the aluminum behaves closer to its intrinsic reflectance, which is why the average over the infrared is five points higher.

The second half of the story is thermal, and it is where the substrate earns its price. Aluminum itself absorbs very little at either end of the specified band, but the optic is not only a coating: it is a 12.0 mm slab of material that absorbs a fraction of the power, sits in a mount that expands differently from it, and lives in an enclosure whose temperature drifts. Zerodur’s coefficient of thermal expansion is 0 ± 0.100 x 10⁻⁶/°C. Fused silica, the material used for the same coating in the standard PF20-03 family, is specified at 0.55 x 10⁻⁶/°C. The ratio is 5.5, and the quantity that ratio multiplies is the temperature difference across the part, not the temperature of the part. A uniformly warmed mirror simply gets slightly larger; a mirror with a gradient across it gets curved, and curvature is what turns watts into pointing error.

Zerodur is a registered trademark of Schott.

Key Features

  • One coating, two band definitions, no gap between them. The 450 nm to 20 µm range is continuous. There is no notch at 2 µm where the specification stops and restarts; the reflectance simply changes slope there, and the two averages describe the two sides of that change. A system that tunes a source from 1.5 µm to 3 µm crosses the boundary without needing a different optic.
  • SiO₂ overcoat, which is a durability decision rather than an optical one. Thorlabs’ description of the protected family applies here directly: the protected gold, silver and aluminum mirrors have a durable SiO₂ overcoat, and each protective overcoat helps to protect the metallic coating from tarnishing and prevents damage to the fragile metallic surface. For aluminum the tarnish mechanism is oxide and hydroxide growth, and the practical consequence is that the G01 can be cleaned with normal laboratory discipline where a bare aluminum surface could not.
  • Ravg of 90 percent from 450 nm to 2 µm and Ravg of 95 percent from 2 to 20 µm. Written as banded averages on purpose. The visible band is where most alignment beams live, and 90 percent is a workable figure for a metal coating that also has to serve the far infrared.
  • Zerodur® substrate with 0 ± 0.100 x 10⁻⁶/°C. The point is not that the mirror never moves; it is that the mirror’s own contribution to the drift budget stays small enough that mount and enclosure effects dominate, which makes the whole system easier to diagnose and to fix.
  • λ/10 at 632.8 nm with 40-20 scratch-dig over a 45.7 mm clear aperture. A two-inch optic with this figure is usable in an interferometer arm as well as in a beam delivery fold, and the 40-20 grade keeps scatter low enough for imaging paths where a bright fold mirror would otherwise put a halo into the field.
  • CW thresholds published at two very different spot sizes. 100 W/cm at 1.070 µm over a Ø0.098 mm spot and 350 W/cm at 10.6 µm over a Ø0.339 mm spot. The numbers look like a factor of 3.5 improvement in the infrared; they are in fact the same intensity limit expressed twice, and the arithmetic is shown in the specifications section below.
  • Engraved identification on the back face. In a multi-wavelength bench where several aluminium-looking mirrors sit in a row, the engraving is the only reliable way to tell a 450 nm to 20 µm part from a 250 nm to 450 nm part once both are in mounts.

Technical Specifications

Parameter Specification
Diameter 50.8 mm (2 in), tolerance +0.0 / -0.1 mm
Thickness 12.0 mm (0.47 in), tolerance ±0.2 mm
Parallelism 3 arcmin or better
Substrate Material Zerodur® (substrate grade)
Coefficient of Thermal Expansion 0 ± 0.100 x 10⁻⁶/°C (fused silica reference: 0.55 x 10⁻⁶/°C)
Part Number PF2011-G01
Coating Protected aluminum
Overcoat SiO₂
Spectral Range 450 nm to 20 µm
Average Reflectance, Visible to SWIR Ravg of 90 percent from 450 nm to 2 µm
Average Reflectance, Mid to Far IR Ravg of 95 percent from 2 to 20 µm
Front Surface Flatness λ/10 at 632.8 nm
Surface Quality 40-20 scratch-dig
Clear Aperture 90 percent of diameter (45.7 mm)
Angle of Incidence 0° to 45°
Back Surface Fine ground, model number laser-engraved
Pulsed Damage Threshold 0.3 J/cm² at 1064 nm, 10 ns, 10 Hz, Ø1.000 mm
CW Damage Threshold (1.07 µm) 100 W/cm at 1.070 µm, Ø0.098 mm
CW Damage Threshold (10.6 µm) 350 W/cm at 10.6 µm, Ø0.339 mm
Typical Mounting Two-inch optic mount or kinematic mount with retaining ring

The damage thresholds are properties of the coating and do not change with the diameter of the optic or with the substrate it sits on; the coating run is the same. They are, however, measured on clean optics, and contamination lowers them substantially, so the useful figure for a production tool is well below the published number.

Now the arithmetic that makes the two CW figures comparable. A CW threshold quoted in W/cm is a linear power density: watts of incident power per centimetre of beam diameter. At 100 W/cm over a Ø0.098 mm beam, the power is about 0.98 W concentrated into an area of 7.5 x 10⁻⁵ cm², which is an intensity near 13,000 W/cm². At 350 W/cm over a Ø0.339 mm beam, the power is about 11.9 W into 9.0 x 10⁻⁴ cm², which is an intensity near 13,100 W/cm². The two specifications describe essentially the same intensity limit. The reason the second number looks 3.5 times larger is that the test spot is 3.46 times larger, and the linear-density convention multiplies by exactly that factor. Anyone who reads 350 W/cm as “this mirror is 3.5 times tougher in the infrared” has misread a unit, not measured a mirror.

Applications

  1. Dual-band benches that switch between visible alignment and infrared work. A helium-neon or 532 nm beam used for set-up, followed by a 3 to 10 µm source for the measurement, is the textbook case for this coating. Both wavelengths stay on the same fold and nobody has to re-align when the source changes.
  2. CO₂ laser beam delivery where a visible pilot beam shares the path. 10.6 µm sits inside the 2 to 20 µm interval at the 95 percent average, and a red pilot beam at 633 nm sits inside the visible interval. One mirror, two beams, no dichroic to align.
  3. Thermal imaging and radiometry. Infrared cameras and blackbody calibration benches fold the optical path several times inside a baffled enclosure, and any drift in the fold moves the image on the focal plane array. A low-expansion substrate keeps the image stable while the enclosure warms up.
  4. Broadband spectroscopy and FTIR sampling accessories. An accessory that has to work from the near infrared into the fingerprint region uses aluminium because no single dielectric stack covers that span at reasonable cost, and the flatness of this substrate keeps the throughput repeatable between scans.
  5. Laser welding and cladding heads with visible camera monitoring. The fold that sends process light to a camera while passing the 1 µm process beam has to survive both the back-reflected process power and the ambient heat of the head; the substrate coefficient decides how much of that heat becomes misalignment.
  6. General-purpose laboratory folding where the source is not yet decided. When a bench is being built for a programme that will change wavelength twice before it ships, a coating that spans three octaves removes a procurement problem before it appears.

Selection Guide

Step 1: fix the two wavelengths, not the band

Write down the shortest and the longest wavelength the optic will ever see. If both fall inside 450 nm to 20 µm, the G01 is a candidate. If the short one is below 450 nm, the G01 is out of specification and the UV-enhanced F01 is the part to look at, accepting that it stops at 450 nm and cannot serve the infrared at all. If the long one is beyond 20 µm, no coating in this family applies and the requirement has moved to a different product line.

Step 2: decide whether 90 percent in the visible is enough

In the visible and near infrared, protected silver (P01) averages 97 percent over the same 450 nm to 2 µm interval, seven percentage points higher, and in a path with several folds that difference compounds. If the visible beam is the one that has to arrive with maximum power, silver is the better coating and the humidity question in the precautions section becomes the deciding constraint. If the visible beam is an alignment beam and the infrared beam carries the energy, aluminium’s lower visible average costs nothing that matters.

Step 3: check whether the infrared band is really 2 to 20 µm

If everything below 800 nm is irrelevant and the work is entirely in the infrared, protected gold (M01) gives 96 percent across 800 nm to 20 µm, a flatter and slightly higher curve over the infrared than aluminium’s 95 percent. Aluminium’s advantage is not the infrared number; it is that the same optic still works at 532 nm.

Step 4: size the aperture and the mount

The clear aperture is 45.7 mm. At 45° incidence the footprint stretches by about 1.41 in one axis, so a beam wider than roughly 32 mm will start to see the edge at the extreme of the specified angle range. On the mount side, a 12.0 mm body is stiff enough for a hand-tightened retaining ring, and the ring should bear outside the clear aperture. Because the substrate expands so little, the mount usually dominates the thermal behaviour: an aluminium mount moves about twenty times more per kelvin than the Zerodur body it holds, so the retaining ring should be compliant enough to let the optic slide rather than be squeezed.

Series Comparison

Seven metallic coatings share this 50.8 mm Zerodur® body. The table lists each coating against the two intervals that matter for a broadband decision, and marks where a coating simply is not specified.

Code Coating Specified Range 450 nm-2 µm 2-20 µm Overcoat
F01 UV-enhanced aluminum 250-450 nm Not specified Not specified MgF₂
G01 Protected aluminum 450 nm-20 µm Ravg 90% Ravg 95% SiO₂
P01 Protected silver 450 nm-20 µm Ravg 97% Ravg 95% SiO₂
M01 Protected gold 800 nm-20 µm Partial band only Ravg 96% over full band SiO₂
M02 MIR enhanced gold 2-20 µm Not specified Ravg 98% SiO₂
M03 Unprotected gold 800 nm-20 µm Partial band only Ravg 97% over full band None
L01 Unprotected gold, line optimised 10.6 µm line Not specified Ravg 99% at the line None

Read the table by column rather than by row. In the 450 nm to 2 µm column the ranking is silver first, aluminium second, and everything else absent; in the 2 to 20 µm column the ranking is the mid-infrared gold first, then the unprotected and protected golds, then silver and aluminium level with each other. Only two coatings appear in both columns, and the G01 is one of them. That is the whole argument for this part: not that it wins any single column, but that it is competitive in both, which is a property no other code in the family has.

FAQ

Q1. My system runs from 532 nm to 10.6 µm. Is the G01 enough?

Yes for coverage, with one caveat about how you read the numbers. 532 nm is inside the 450 nm to 2 µm interval, so the 90 percent average applies to the band that contains it. 10.6 µm is inside the 2 to 20 µm interval, so the 95 percent average applies there. Both wavelengths are inside the specified range, the coating is the same film at both, and the only thing that changes is which average you quote. The caveat is that neither average is a value at a specific wavelength: if your link budget needs the actual reflectance at 532 nm or at 10.6 µm rather than the band average, ask us for the measured curve before you commit, because a band average can sit a few points above or below any single line inside the band.

Q2. Is the protected aluminum better than protected silver for humid environments?

Aluminum is less sensitive to humidity than silver, because the failure mechanism for silver is chemical and for aluminum it is not, but the SiO₂ overcoat on this part should still not be relied on as a humidity barrier. The overcoat is a thin dielectric film, not a hermetic seal, and water vapour will reach the metal through pinholes and at the coating edge given enough time and enough cycling. Treat the G01 as an optic for a dry enclosure or a conditioned laboratory, and treat any statement that a protected metal mirror is immune to humidity as marketing rather than engineering.

Q3. What happens to the reflectance at 45° compared with normal incidence?

Aluminium is a metal, so the reflectance changes smoothly with angle and there is no interference notch to fall into. The specified range of 0° to 45° means the coating is characterised across that span, not that it is tuned to one angle. What changes at 45° is the polarization split, which grows with angle, and the footprint, which stretches by about 1.41 along one axis. A path with an odd number of 45° folds will therefore rotate the polarization of a linearly polarized beam, which matters for a polarization-sensitive experiment and does not matter for a welding head.

Q4. Can I use the G01 below 450 nm, for example at 405 nm?

The coating is not specified there and you should not design around it. Aluminium is still reflective at 405 nm, but the protected aluminium design is optimised for 450 nm and up, and the SiO₂ overcoat begins to absorb toward the blue end of the ultraviolet. If 405 nm is a real requirement, the UV-enhanced F01 covers 250 nm to 450 nm with an MgF₂ overcoat and an average of 90 percent, and it is the correct part even though it gives up the infrared entirely. If both 405 nm and 10.6 µm are genuinely needed in the same path, the honest answer is two mirrors on a flip mount rather than one mirror that is out of specification at one end.

Q5. The pulsed threshold is quoted at 1064 nm with a 1 mm spot. Is that a large-spot or a small-spot test?

A 1.000 mm test spot is a large-spot measurement, which is the conservative kind for defect-initiated damage: the larger the spot, the higher the probability that the beam covers a defect that initiates failure, so a large-spot threshold is generally lower than a small-spot one for the same coating. A value of 0.3 J/cm² measured that way is a realistic ceiling for nanosecond pulses rather than an optimistic one. If your beam is much smaller than 1 mm, the fluence limit still applies but the statistics change, and if your pulses are shorter than 10 ns the threshold will move in a way that only a measurement at your pulse duration can settle.

Q6. Why does the coating stop at 20 µm instead of going further into the far infrared?

Because beyond 20 µm the specified performance is no longer what the design was qualified for, and the phonon absorption bands of the dielectric overcoat start to matter more than the metal’s reflectance. The aluminium film itself would still reflect well beyond that point, but the SiO₂ layer in front of it would not, and the published average of 95 percent applies only to the 2 to 20 µm interval. If a terahertz or long-wave infrared requirement appears, the answer is a different coating family, not an extrapolation of this one.

Usage Precautions

  • Clean only when there is something to remove. The SiO₂ overcoat survives normal solvent cleaning, but every wipe is an opportunity to leave a residue or a sleeker mark. Blow off loose dust with clean dry air or nitrogen first, and clean with solvent only if the surface still shows a film.
  • Never drag a dry tissue across the coating. Flood with clean solvent, drag a lens tissue once in a single direction under its own weight, and stop. A dry drag on a coated metal surface generates enough local friction to damage the overcoat, and the damage is not repairable.
  • Do not treat the overcoat as a humidity barrier. Store the part in its case in a dry environment, and if the bench runs in a humid room, keep the optic in a purged or desiccated enclosure. Aluminum is more forgiving than silver here, but a thin dielectric film is not a seal.
  • Keep the mount compliant in the radial direction. With a substrate this dimensionally stable, the mount is usually the larger thermal term. A rigid clamp on an aluminium body will impose its own expansion on a Zerodur optic, and the resulting figure error will look exactly like a bad mirror.
  • Do not exceed the published fluence during set-up. Alignment often runs the laser at full power into a small spot on a fold mirror, which is precisely the condition the damage threshold table warns about. Use a beam block or a pick-off for alignment, and check the fold after any change to the beam size.
  • Handle by the edge with gloves, and never touch the coated face. A fingerprint on a protected aluminium mirror is removable in principle and a permanent cosmetic defect in practice, because the cleaning that removes it also works on the overcoat.

Disclaimer

Specifications on this page are compiled from Thorlabs’ publicly published product documentation and are provided for selection reference only. If this page and the manufacturer’s current official datasheet disagree, the datasheet governs. Specifications, coatings and appearance may change without notice. Damage thresholds are measured values under the test conditions stated and are not a guarantee of performance in any particular system; verifying suitability at your own wavelength, fluence, pulse duration and beam size is the user’s responsibility. Prices and delivery times are confirmed by our sales team at quotation.

Contact Us

Tell us the shortest and longest wavelength in your path, the number of folds and the beam diameter, and we will tell you whether a broadband aluminium coating is the right answer or whether the band should be split across two optics.

Hotline: +86 159-2722-0467

E-mail: 859818709@qq.com  |  Website: www.soar-laser.cn

Evaluation units and volume orders are both available, and the same coating can be quoted in Ø1/2 in and Ø1 in versions from the same family.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF2011-G01 Ø50.8 mm (2 in) Zerodur® Protected Aluminum Mirror, 450 nm – 20 µm”

Your email address will not be published. Required fields are marked *

中文EN