Description
Product Overview
The Thorlabs PF07-03-G01 is the general-purpose member of the Ø19.0 mm group: a fused silica plano mirror, 6.0 mm thick, coated with aluminium and sealed under a silica overcoat, specified above 90% average reflectance from 450 nm to 2 µm and above 95% from 2 to 20 µm. It holds the highest reflectance of nothing in the catalogue and the lowest price of everything here, which is exactly why it is the mirror most often bolted into a layout and forgotten.
The case for protected aluminium is not that it wins a specification contest. It is that aluminium is cheap, reflects reasonably from the visible into the far infrared, and can be sealed well enough to be handled. The silica overcoat does two things: it keeps the soft metal away from fingers and cleaning solvents, and it slows the tarnish that attacks an unprotected film. Thorlabs states that the protected aluminium coating has a smaller chance of tarnishing than protected silver in a high humidity environment, and that its reflectance most closely matches that of a bare aluminium coating. Those two sentences describe its real niche: an optic for rooms and machines where nobody is going to look after it.
The compromises are honest ones. In the visible, aluminium sits roughly five points below silver, which is visible as a slightly dimmer reflection and matters in a low-light imaging path but not in a beam dump or a fold. In the infrared, gold is a point or two higher and, more importantly, flatter, because aluminium carries its own interband absorption structure near 800 nm while gold does not. And there is no ultraviolet: the specification starts at 450 nm, and below that a different film is needed.
The 19 mm diameter exists for the Polaris fixed mount, and a general-purpose fold is the duty that mount was designed for. A mirror that is installed once and left alone does not need a kinematic stage; it needs a seat that does not move. The POLARIS-19S50/M holds a 6 mm thick, 19 mm optic with a three-point flexure contact in a Ø1 inch footprint, which is cheaper and more stable than a two-axis adjuster doing a job that requires no adjustment.
Key Features
- Silica-sealed aluminium: the overcoat makes the film wipeable and slows tarnish, giving the best humidity tolerance of any coating in this group
- Two-plateau reflectance: above 90% from 450 nm to 2 µm and above 95% from 2 to 20 µm, so one part spans the visible, near infrared and most of the mid infrared
- Closest match to bare aluminium: the seal adds little, which keeps the reflectance curve predictable if a layout was designed around an uncoated film
- Lowest cost of the five coatings: the practical reason it appears in quantity in OEM builds and in teaching laboratories
- Published thresholds: 0.3 J/cm² at 1064 nm with 10 ns pulses at 10 Hz, and CW ratings of 100 W/cm at 1.070 µm and 350 W/cm at 10.6 µm
- Ø19.0 mm x 6.0 mm: λ/10 figure at 633 nm, 40-20 scratch-dig, parallelism within 3 arcmin, clear aperture 90% of the diameter
Technical Specifications
| Model | PF07-03-G01 |
| Coating | Protected aluminium |
| Overcoat | Silica (SiO₂) |
| Wavelength range | 450 nm – 20 µm |
| Average reflectance | above 90% from 450 nm to 2 µm; above 95% from 2 to 20 µm |
| Substrate | Fused silica |
| Diameter | Ø19.0 mm (0.75 in) |
| Diameter tolerance | +0.0 mm / -0.1 mm |
| Thickness | 6.0 mm (0.24 in) |
| Thickness tolerance | +/-0.2 mm |
| Clear aperture | 90% of diameter, about Ø17.1 mm |
| Surface flatness | λ/10 peak to valley at 633 nm |
| Surface quality | 40-20 scratch-dig |
| Parallelism | at most 3 arcmin |
| Pulsed damage threshold | 0.3 J/cm² at 1064 nm (10 ns, 10 Hz, Ø1.000 mm) |
| CW damage threshold | 100 W/cm at 1.070 µm (Ø0.098 mm); 350 W/cm at 10.6 µm (Ø0.339 mm) |
| Humidity behaviour | less prone to tarnish than protected silver in high humidity |
| Cleanable | Yes, with care |
| Source | Thorlabs official series specification table |
Applications
Because the band runs from the visible to the far infrared, this is the optic that gets specified when the source is not yet fixed, or when the same bench has to serve several lasers on different days. The four situations below are where it earns its place rather than merely doing the job.
- General optical bench folding: periscopes, delay arms and beam-height changes where the wavelength may change later and a wideband metal film avoids a redesign
- Teaching and prototype builds: student laboratories and first-article rigs, where optics are handled often, cleaned carelessly and replaced on a budget
- Low and medium power industrial delivery: turning a marking or welding beam between the source and the head at power densities inside the 100 to 350 W/cm CW ratings
- Multi-wavelength benches: a visible alignment laser and an infrared working beam sharing the same fold, where a coating optimised for one of them would leave the other unserved
Selection Guide
- Start here unless a number says otherwise: if the band is 450 nm to 20 µm and the power is moderate, protected aluminium is the default and the other four coatings are the exceptions, each bought for a specific reason
- Move to silver only for visible throughput: the gain is about five percentage points in the visible and near infrared. That is worth paying for in an imaging or display path and rarely worth it in a fold where the beam is dumped afterwards
- Move to gold above 800 nm: not so much for the extra point or two as for the flat curve, which matters when the band is wide or the source drifts
- Do not push it into the ultraviolet: the specification begins at 450 nm. A 405 nm or 355 nm beam needs the UV-enhanced coating, and a 450 nm beam sits exactly on the boundary where neither coating is at its best
- Count the mirrors before choosing: at 90% per reflection, ten folds leave 35% of the beam. If the layout has many reflections, the extra cost of silver or gold is repaid quickly, and if it has two, it is not
Series Comparison
The table below puts the same 19 mm substrate and mount against the alternative films, with the columns ordered the way a purchasing decision is actually made: what it costs, and what it survives.
| Item | Coating | Wavelength range | Average reflectance | Relative cost | Humidity tolerance |
| PF07-03-G01, this page | Protected aluminium | 450 nm – 2 µm; 2 – 20 µm | 90% / 95% | Lowest | Best of the group |
| PF07-03-P01 | Protected silver | 450 nm – 2 µm; 2 – 20 µm | 97% / 95% | Higher | Tarnishes faster, avoid high humidity |
| PF07-03-M01 | Protected gold | 800 nm – 20 µm | 96% | Higher | Good |
| PF07-03-M02 | MIR-enhanced gold | 2 – 20 µm | 98% / 95% absorption-weighted | Highest | Good, MIL-C-48497A overcoat |
| PF07-03-F01 | UV-enhanced aluminium | 250 – 450 nm | above 90% | Comparable | MgF₂ cap, keep dry |
Smaller diameters of the same coating are stocked for compact hardware: a Ø1/2 inch protected aluminium mirror and the low-expansion Zerodur protected aluminium mirror for thermally demanding benches.
FAQ
Should I order the G01 or the P01? Order the G01 if the layout is broadband, the power is moderate and the mirror will be handled. Order the P01 if every photon in the visible matters, for example in an imaging relay or a display engine. The difference is about five percentage points per reflection between 450 nm and 2 µm, and the protected aluminium is the more forgiving of the two in a humid room.
Why is the visible reflectance only about 90% when silver reaches 97%? Because aluminium is a poorer reflector than silver in that band; it is not a coating defect. The silica seal is also slightly absorbing compared with the bare metal, which is why Thorlabs describes this coating as the one that most closely matches bare aluminium rather than as the brightest.
Can it be used at 405 nm? Not within specification. The coating is characterised from 450 nm, and below that the aluminium plus its oxide starts to lose reflectance quickly. For 405 nm or shorter, use the UV-enhanced aluminium item, which is specified from 250 nm.
Is it safe to clean? Yes, with care. The silica overcoat is hard enough to survive a standard solvent and tissue procedure, unlike the UV-enhanced coating. Blow off grit first, use reagent-grade solvent on a lens tissue, and drag in one direction rather than scrubbing in circles.
Is 0.3 J/cm² enough for a Q-switched 1064 nm laser? It depends entirely on the beam area at the mirror. A 10 ns pulse of 30 mJ spread over a 4 mm diameter is roughly 0.24 J/cm² and sits below the threshold; the same energy focused to 1 mm is about 3.8 J/cm² and will damage the coating. Calculate the fluence at the surface, not the output energy of the laser.
Usage Precautions
- Clean less often than you think: the silica overcoat tolerates cleaning, but every wipe carries a small risk. Blow off dust with dry gas first and reserve solvent cleaning for contamination that will not lift
- Keep the beam inside the clear aperture: 90% of 19.0 mm leaves about 17 mm. A beam that clips the edge of a metal coating produces scatter and, at higher power, a damaged rim that grows inward
- Respect the CW ratings as linear power density: 100 W/cm at 1.070 µm means the power divided by the beam diameter in centimetres, not the power per square centimetre. A tight focus is what exceeds this rating
- Seat the optic flat: the back face is fine ground and sits on the mount seat. Grit between the seat and the optic tilts the mirror and, on a 6 mm substrate, bends it
- Store dry but not sealed wet: a case with desiccant is right; wrapping the optic in a solvent-soaked tissue is not. Residue trapped against the coating under a wrap is a common cause of a hazy mirror
- Mark the coated face: both faces look similar under room light. The coated face is the one that shows a sharp reflection; the back is fine ground and engraved with the part number
Disclaimer
Specifications on this page are compiled from Thorlabs official published material and are provided as a selection reference. The current official specification sheet governs; specifications and appearance may change without notice. Price and lead time are quoted by our sales team on request.
Contact Us
Changsha Soar Laser Equipment Co., Ltd. holds stock of Thorlabs metallic mirrors and can advise on coating choice for a specific source and power level. Call +86 159 2722 0467, write to 859818709@qq.com, or visit www.soar-laser.cn for the full range.