Description
Product Overview
The PF0511-G01 is a 12.7 mm Zerodur disc carrying the protected aluminum coating: aluminum with a silicon dioxide overcoat, specified at an average reflectance of 90% from 450 nm to 2 µm and 95% from 2 µm to 20 µm. The disc is 6.0 mm thick with a tolerance of plus or minus 0.2 mm, flat to lambda/10 peak to valley at 632.8 nm, polished to 40-20 scratch-dig, parallel to within 3 arcmin, and figured so that the clear aperture reaches 90% of the diameter. The item number is engraved on the fine-ground back face.
The substrate is the reason this part exists next to the cheaper fused silica PF05-03-G01. Zerodur is a glass-ceramic made by Schott, and the registered trademark is Schott’s; Thorlabs buys it in substrate grade. Its coefficient of thermal expansion is 0 plus or minus 0.100 x 10-6/degC, against 0.55 x 10-6/degC for fused silica, which is a factor of five and a half. A 10 K swing across a workshop therefore moves the surface about five times less. On a 12.7 mm part that sounds academic, until the mirror sits at the far end of a two-metre beam path and the return beam has to land back inside a 50 um spot.
Aluminum is the least expensive way to span 450 nm to 20 µm with one coating, and the overcoat is what makes it a usable industrial part rather than a laboratory curiosity: it protects a metal that is otherwise soft and quick to oxidise. Thorlabs states that the protected aluminum coating has a smaller chance of tarnishing than protected silver in a high humidity environment, and that its reflectance curve most closely follows that of bare aluminum. The price of that breadth is efficiency: 90% in the visible means one bounce costs you a tenth of the beam, and four bounces cost a third.
Two boundaries are worth stating plainly. Below 450 nm this coating is out of band and the UV-enhanced aluminum -F01 takes over at 90% from 250 nm to 450 nm. Where the visible budget cannot absorb a 10% loss per reflection, protected silver -P01 buys seven points at the cost of humidity tolerance. The uncoated PF0511 Zerodur blank is the starting point if you intend to specify your own coating.
Key Features
- Zerodur substrate: 0 plus or minus 0.100 x 10-6/degC, five times stiffer against thermal drift than fused silica
- Protected aluminum: average reflectance 90% from 450 nm to 2 µm and 95% from 2 µm to 20 µm, one coating for the visible through the far infrared
- Silicon dioxide overcoat: a hard, cleanable layer over a metal that would otherwise mark at the first touch
- Humidity tolerance: Thorlabs rates its tarnish resistance above that of protected silver in damp environments
- Surface figure: lambda/10 peak to valley at 632.8 nm, 40-20 scratch-dig, parallelism 3 arcmin maximum, clear aperture 90% of the diameter
- 0 to 45 degree incidence: the coating is specified across the folding angles used in real beam-delivery hardware, not only at normal incidence
Technical Specifications
| Parameter | Value |
|---|---|
| Item Number | PF0511-G01 |
| Coating | Protected Aluminum (aluminum plus SiO2 overcoat) |
| Wavelength Range | 450 nm to 20 µm |
| Average Reflectance | 90% from 450 nm to 2 µm; 95% from 2 µm to 20 µm |
| Angle of Incidence | 0 to 45 degrees |
| Substrate | Zerodur (Schott registered trademark, substrate grade) |
| Diameter | 12.7 mm (1/2 inch), +0.0 / -0.1 mm |
| Thickness | 6.0 mm (0.24 inch), plus or minus 0.2 mm |
| Clear Aperture | 90% of the diameter |
| Front Surface Flatness | lambda/10 peak to valley at 632.8 nm |
| Surface Quality | 40-20 scratch-dig |
| Parallelism | 3 arcmin maximum |
| Coefficient of Thermal Expansion | 0 plus or minus 0.100 x 10-6/degC (fused silica reference: 0.55 x 10-6/degC) |
| Back Surface | Fine ground, item number engraved |
| Pulsed Damage Threshold | 0.3 J/cm2 at 1064 nm, 10 ns, 10 Hz, over 1.000 mm |
| CW Damage Threshold | 100 W/cm at 1.070 µm over 0.098 mm; 350 W/cm at 10.6 µm over 0.339 mm |
| Source | Thorlabs official series specification table |
The two damage-threshold rows are the coating-level ratings Thorlabs publishes for the -G01 coating in its optical coatings table. The film here is the same film, so the numbers carry over, but a rating is a starting point and not a warranty: your beam diameter, pulse length, repetition rate and duty cycle decide what the part will actually survive.
Applications
- Gantry and galvo heads on marking or cutting machines: the fold mirrors sit closest to the heat source and drift first, which is exactly where a low-expansion substrate earns its premium over a glass disc
- Beam-delivery risers and periscopes: two or three 45 degree reflections in series multiply angular error, so substrate stability matters more than the last percent of reflectance
- Broadband laboratory folds: one coating that still works when the source is swapped from a 532 nm DPSS to a 10.6 µm CO2 tube without touching the mount
- Machine-vision illumination relays: white-light paths where a 90% mirror is acceptable because the camera is not photon-starved
- OEM instruments: cost-driven builds that need a documented, repeatable substrate rather than the best possible reflectance
Selection Guide
Work through these five questions in order; the first one that fails eliminates the part.
- Is the wavelength inside 450 nm to 20 µm? Below 450 nm, stop here and take the -F01 UV-enhanced aluminum coating instead.
- Will the optic live in a damp or uncleaned environment? If yes, aluminum is the safer of the two broadband metals; protected silver tarnishes faster in humidity even with its overcoat.
- Can the power budget absorb 10% per reflection? If the answer is no and the band is 450 nm to 2 µm, the silver -P01 is the correct upgrade.
- Does the beam path amplify drift? Long arms, double passes and interferometric readout justify Zerodur; a short bench does not, and the fused silica version saves money.
- Is the beam inside 90% of the diameter? A 12.7 mm optic with 11.4 mm of clear aperture is the practical limit; clipping the edge puts scatter straight back into the return path.
Series Comparison
All five coatings below are offered by Thorlabs on the same PF0511 Zerodur body, so the mechanical envelope, figure and finish are identical and only the film changes.
| Coating | Wavelength Range | Average Reflectance | Where It Wins |
|---|---|---|---|
| -F01 UV Enhanced Aluminum | 250 nm to 450 nm | 90% | Ultraviolet only; below the aluminum band used here |
| -G01 Protected Aluminum | 450 nm to 20 µm | 90% / 95% | Widest band per unit cost, best humidity behaviour |
| -P01 Protected Silver | 450 nm to 20 µm | 97% / 95% | Visible and near infrared efficiency |
| -M01 Protected Gold | 800 nm to 20 µm | 96% | Infrared from 800 nm up, cleanable |
| -M03 Unprotected Gold | 800 nm to 20 µm | 97% | Polarization purity and the far infrared |
FAQ
Is protected aluminum good enough in a humid workshop? Better than protected silver, which is the comparison Thorlabs itself draws: the aluminum coating has a smaller chance of tarnishing in high humidity. It is not sealed, though. If the machine sits in an unheated space with condensation cycles, the overcoat will eventually haze, and no coating on this page is rated for that.
How do I clean it? The SiO2 overcoat is hard enough for a normal solvent drag wipe: blow off loose dust first, then use reagent-grade solvent and a lens tissue drawn once across the surface, never a dry rub. The point of the overcoat is that this is allowed at all; the unprotected gold -M03 on the same substrate forbids every method except blowing dust off.
Why only 90% when silver reaches 97%? Aluminum has a plasma edge in the deep ultraviolet and its reflectance climbs through the visible; silver is already near its peak at 450 nm. The trade is deliberate: aluminum holds a usable curve all the way to 20 µm and tolerates humidity, silver is seven points brighter over the visible and near infrared and is the more delicate film of the two.
Do I need Zerodur, or is the fused silica version fine? Fused silica at 0.55 x 10-6/degC is fine for a bench that stays within a few degrees and a beam path under a metre. Zerodur at 0 plus or minus 0.100 x 10-6/degC is the answer when the optic is bolted to a machine frame that heats up, or when the return beam has to survive several reflections without walking off the detector.
Usage Precautions
- Hold the optic by the rim, with gloves or finger cots. A fingerprint on a coated mirror is a localised absorber and, at power, a localised failure point.
- Never dry-wipe a surface that may carry grit. Blow first, then wipe wet, then wipe once with a clean tissue and stop.
- Do not over-clamp. A retaining ring tightened until it feels secure is already enough to bend a 6 mm disc and print astigmatism into the reflected wavefront.
- Keep the beam inside the 90% clear aperture. The last millimetre of a mirror is where edge scatter and figure roll-off live.
- Include the 10% loss in the power budget. At 100 W through three folds, roughly 27 W becomes heat in the mounts, and that heat is what the Zerodur substrate was bought to survive.
Disclaimer
Specifications on this page are transcribed from Thorlabs official public documentation and are provided for selection reference only. The current official specification sheet governs. Thorlabs may change specifications, coatings and appearance without notice. Prices, availability and delivery times are confirmed by our sales team at the time of order; nothing on this page is a binding offer.
Contact Us
Gaofei Laser supplies genuine Thorlabs stock and can quote this item with current availability, lead time and volume pricing. Send the item number, the quantity you need and the wavelength you are working at, and we will confirm the coating, the substrate and the mounting interface before you order.
- Sales hotline: +86 159 2722 0467
- Email: 859818709@qq.com
- Website: www.soar-laser.cn









Reviews