Product Overview

The PF0511-F01 is a Ø12.7 mm (Ø1/2 inch) mirror carrying Thorlabs UV enhanced aluminum on a Zerodur substrate. Average reflectance is 90% from 250 nm to 450 nm, the disc is 6.0 mm thick, the front face is figured to λ/10 at 632.8 nm and polished to 40-20 scratch-dig, parallelism is inside 3 arcmin, and clear aperture is 90% of the diameter. Diameter tolerance is +0.0 / -0.1 mm and thickness tolerance is ±0.2 mm. The item number is engraved on the back.

Two decisions are stacked in this part number, and they answer two different problems. The first is the film: below roughly 450 nm silver stops being a good reflector, because the interband absorption that sits far in the ultraviolet for silver moves into the working band and the reflectance falls away steeply. Aluminum does not have that problem. Its useful reflectance reaches down toward 200 nm, which is why every ultraviolet metal mirror in a catalogue is aluminum and not silver. The second decision is the substrate: Zerodur, for the thermal stability, and that is what separates this part from the same coating on fused silica.

The overcoat is what makes the aluminum usable rather than merely reflective. Bare aluminum grows a native oxide within seconds of deposition, and that oxide absorbs strongly in the deep ultraviolet, which is exactly the region the mirror is bought for. Thorlabs deposits an MgF₂ overcoat on its UV enhanced aluminum instead of the SiO₂ used on the protected coatings. MgF₂ is transparent far into the ultraviolet, so it protects the metal without eating the band it is meant to serve, and the result is the 90% average over 250 nm to 450 nm that defines the -F01 suffix. The same MgF₂ layer is softer than an SiO₂ overcoat, which has a direct consequence for cleaning.

The substrate argument is the low expansion coefficient. Zerodur is 0 plus or minus 0.100 x 10 to the minus 6 per degree Celsius against 0.55 for fused silica, a factor of five and a half. Ultraviolet systems are often high average power systems: a tripled Nd:YAG at 355 nm, an excimer at 308 nm, a frequency-quadrupled source at 266 nm. Absorption in the film and in the substrate turns average power into heat, heat turns into a thermal gradient across a 12.7 mm disc, and a gradient across a disc with a large expansion coefficient bends the surface. A substrate that barely expands removes one term from that chain. On this part, a 20 K swing moves the dimension by about 25 nm where fused silica would move about 140 nm.

Thorlabs publishes laser damage figures for the -F01 coating that are worth reading carefully because the test spots are small: 0.25 J/cm² at 266 nm for 10 ns pulses at 10 Hz over Ø0.150 mm, and 0.3 J/cm² at 355 nm for 10 ns at 10 Hz over Ø0.381 mm. The CW entries are 300 W/cm at 1.064 µm over Ø0.044 mm and 500 W/cm at 10.6 µm over Ø0.339 mm. Those spots are far smaller than a real beam, so the figures should be scaled by beam area and treated as coating level data rather than as a guarantee for a particular optical layout. They are still the numbers to start from when a 355 nm beam has to be folded at power.

Key Features

  • UV enhanced aluminum, 90% average from 250 nm to 450 nm, the band where silver reflectance has already collapsed
  • MgF₂ overcoat rather than SiO₂: transparent far into the ultraviolet, so it protects the aluminum without absorbing the band it is specified for
  • Zerodur substrate at 0 plus or minus 0.100 x 10 to the minus 6 per degree Celsius, five and a half times more stable than fused silica at 0.55
  • Built for high average power ultraviolet: substrate heating that would bend a fused silica disc barely moves a Zerodur one
  • λ/10 peak to valley at 632.8 nm with 40-20 scratch-dig and parallelism inside 3 arcmin
  • 12.7 mm diameter by 6.0 mm thick, tolerances +0.0 / -0.1 mm and ±0.2 mm, clear aperture 90% of the diameter
  • Coating level laser data published: 0.25 J/cm² at 266 nm and 0.3 J/cm² at 355 nm, both for 10 ns pulses at 10 Hz
  • Engraved item number on the back face, and a mount interface identical to the fused silica version so the two are interchangeable

Technical Specifications

Parameter Value
Model PF0511-F01
Coating UV enhanced aluminum with MgF₂ overcoat
Wavelength range 250 nm – 450 nm
Average reflectance 90% from 250 nm to 450 nm
Substrate Zerodur glass-ceramic, substrate grade (registered trademark of Schott)
Coefficient of thermal expansion 0 ± 0.100 x 10^-6 per degree Celsius, against 0.55 for fused silica
Diameter 12.7 mm (Ø1/2 inch)
Diameter tolerance +0.0 mm / -0.1 mm
Thickness 6.0 mm (0.24 inch)
Thickness tolerance ±0.2 mm
Front surface flatness λ/10 at 632.8 nm
Surface quality 40-20 scratch-dig
Parallelism 3 arcmin or less
Clear aperture 90% of the diameter
Damage threshold, pulsed 0.25 J/cm² at 266 nm, 10 ns, 10 Hz, Ø0.150 mm; 0.3 J/cm² at 355 nm, 10 ns, 10 Hz, Ø0.381 mm
Damage threshold, CW 300 W/cm at 1.064 µm, Ø0.044 mm; 500 W/cm at 10.6 µm, Ø0.339 mm
Source Thorlabs official series specification table

Applications

Ultraviolet folding is a narrow niche with its own failure modes: the film choice is forced, the power is often high, and the optics are frequently the cheapest part of an expensive experiment. These are the layouts where this part belongs.

  • 355 nm tripled Nd:YAG beam delivery: harmonic separation, beam expansion and focus-head folding, where the third harmonic is generated at high average power and the fold train sits downstream of the heat
  • 266 nm frequency-quadrupled sources: the fourth harmonic is where coating absorption and substrate heating both peak, and the low expansion substrate is doing the most work
  • Ultraviolet interferometry: a reference fold at 355 nm or 266 nm in a setup that must hold fringe position through a warm-up, not just at switch-on
  • Excimer laser annealing and marking: 308 nm XeCl and 248 nm KrF lines folded into a line generator, where pulse energy and repetition rate both load the coating
  • Lithography and mask inspection relay optics: ultraviolet illumination paths where a fold that drifts shows up as an alignment offset across a field
  • Ultraviolet fluorescence and Raman excitation paths: folding a 266 nm or 325 nm excitation line without adding a thermal drift term to a measurement that runs for hours

Selection Guide

The wavelength decides the film before anything else does, and the crossover is sharper than most buyers expect.

Coating Band Average reflectance Verdict for ultraviolet work
UV enhanced aluminum, -F01 250 nm – 450 nm 90% The only metal coating specified in this range; MgF₂ keeps the band open
Protected aluminum, -G01 450 nm – 20 µm 90% / 95% Its SiO₂ overcoat absorbs below about 450 nm, so it is the wrong film for a UV fold
Protected silver, -P01 450 nm – 20 µm 97% / 95% Highest visible figure, but reflectance collapses below 450 nm; never a UV choice

The crossover that matters is between 400 nm and 450 nm. A 405 nm diode is a marginal case that depends on how much loss the link can absorb; a 355 nm or 266 nm line is unambiguous and needs this coating. The trade is that below 450 nm there is no higher-reflectance metal option at all, so the 90% figure is not a compromise against a better alternative, it is the ceiling. If more than 90% is genuinely required, the answer is a dielectric stack designed for the exact line, not a metal film.

Between this part and the fused silica PF05-03-F01 the coating is identical and the envelope is identical, so the choice is purely thermal against cost. If the ultraviolet power is low, or the mount already dominates the drift budget, the fused silica part does the same optical job for less. If the system runs at power and must hold alignment through a warm-up, the Zerodur substrate is the reason to pay more.

Series Comparison

Zerodur is available under five metal coatings, and the table shows why the ultraviolet one is a different animal from its stablemates rather than simply another suffix.

Item number Coating Band Average reflectance Overcoat
PF0511-F01 UV enhanced aluminum 250 nm – 450 nm 90% MgF₂
PF0511-G01 Protected aluminum 450 nm – 20 µm 90% / 95% SiO₂
PF0511-P01 Protected silver 450 nm – 20 µm 97% / 95% SiO₂
PF0511-M01 Protected gold 800 nm – 20 µm 96% Dielectric
PF0511-M03 Unprotected gold 800 nm – 20 µm 97% None

All five share the same Zerodur substrate, the same 12.7 mm by 6.0 mm envelope, the same λ/10 figure and the same 3 arcmin parallelism, so the low expansion benefit is common to the family and only the film changes. The F01 is the only one whose overcoat is MgF₂, and the only one specified below 450 nm. The M03 has no overcoat at all, which is the opposite extreme: highest reflectance in the infrared, no tolerance for handling. Reading down that column is the fastest way to see that overcoat chemistry, not substrate, is what sets the band.

The uncoated PF0511 Zerodur mirror blank is the same substrate before any of these films are applied, for customers whose band is not on this list.

FAQ

Why aluminum and not silver at 355 nm? Because silver reflectance falls steeply below about 450 nm as interband absorption moves into the band, while aluminum holds its reflectance down toward 200 nm. For an ultraviolet fold there is no silver option to weigh.

What does the MgF₂ overcoat actually do? It seals the aluminum against the native oxide that would otherwise form and absorb in the deep ultraviolet, and it is itself transparent far into the ultraviolet. The SiO₂ used on the protected coatings would absorb in exactly the region this mirror is bought for.

How does it compare with the fused silica UV enhanced aluminum mirror? Same coating, same 12.7 mm by 6.0 mm envelope, same λ/10 and 40-20, so they are interchangeable in a mount. The difference is the expansion coefficient, 0 plus or minus 0.100 against 0.55, and the price. Choose on thermal requirement, not on optical performance.

Can it be cleaned? Yes, with standard solvent and lens tissue procedure, but gently. MgF₂ is softer than an SiO₂ overcoat and more easily damaged by abrasion, so lift contamination with solvent rather than wiping a dry surface, and never use a dry lens cloth on a dusty face.

What is the laser damage limit at 355 nm? Thorlabs quotes 0.3 J/cm² for 10 ns pulses at 10 Hz over a Ø0.381 mm spot, and 0.25 J/cm² at 266 nm over Ø0.150 mm. Both spots are small, so scale by beam area and send us the actual beam diameter and repetition rate if the margin looks thin.

Does the substrate really matter if the coating absorbs the light? It matters more, not less. Absorption becomes heat, heat becomes a gradient, and a gradient across a disc bends it in proportion to the expansion coefficient. A low expansion substrate removes the last term in that chain, which is the term you cannot fix with a better mount.

Is the clear aperture smaller because of the coating? No. Clear aperture is 90% of the diameter on every part in this family, coated or not. The remaining annulus is where a mount should grip.

Usage Precautions

  • Handle by the edge with gloves and keep the coated face covered when the optic is out of its container
  • Clean with solvent and lens tissue only, lifting contamination rather than wiping a dry surface; the MgF₂ overcoat is softer than SiO₂
  • Never dry-wipe, and never use abrasive tissue, polishing compound or ultrasonic cleaning on this coating
  • Avoid prolonged exposure of the coated face to organic contamination under ultraviolet illumination, which can bake a fingerprint into the film permanently
  • Keep the optic dry and free of water spots; MgF₂ is more sensitive to moisture than an SiO₂ overcoat
  • Assess any beam above the published test conditions from actual beam diameter and pulse duration rather than scaling the table directly
  • Seat with light retaining-ring pressure, since a 6.0 mm disc distorts under a ring tightened by feel and the λ/10 figure is the thing being protected

Disclaimer

Specifications are transcribed from the Thorlabs metallic Zerodur mirror specification table and the Thorlabs broadband high reflectance coating specification table for selection purposes. The damage threshold figures are coating level values published for the -F01 coating over the small test spots stated, and they are not a guarantee for any particular optical layout; the official datasheet in force at the time of purchase governs. Reflectance values are averages over 250 nm to 450 nm, and performance outside that band is typical rather than guaranteed. Price and lead time are quoted by our sales team against live stock.

Contact Us

Changsha Soar Laser Equipment Co., Ltd. supplies genuine Thorlabs optics to laboratories and machine builders in China. Ultraviolet folds are usually specified late, under time pressure, after the harmonic generator has already been chosen, so the useful question is short: what is the wavelength, what is the average power, and how much drift can the experiment tolerate between alignments. Send those three and we will tell you whether this part is right or whether the fused silica version will do. Hotline +86 159 2722 0467, email 859818709@qq.com, website www.soar-laser.cn.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF0511-F01 Ø1/2″ Zerodur UV Enhanced Aluminum Mirror, 250-450 nm”

Your email address will not be published. Required fields are marked *

中文EN