Description

Product Overview

The PF20-03-F01 is a 50.8 mm (2 in) diameter, 12.0 mm thick ultraviolet mirror from Thorlabs, built on a fused silica substrate and finished with a UV-enhanced aluminum coating that carries an MgF2 overcoat. Its specified band is 250 to 450 nm, its guaranteed average reflectance is 90 percent, and its surface figure is lambda/10 peak-to-valley measured at 633 nm. It is the optic you reach for when a beam is too short in wavelength for the ordinary protected aluminum mirror to be trusted, and too broadband for a narrowband dielectric stack to be affordable.

An ultraviolet mirror is a chemistry problem before it is a coating design problem

Aluminum has one of the highest intrinsic reflectances of any practical metal in the ultraviolet, which is why almost every UV mirror ever made starts with aluminum rather than with silver or gold. The difficulty is not optical, it is chemical. A freshly deposited aluminum film is unstable in air: an oxide skin begins to form on it within seconds of exposure, and that skin absorbs strongly in the ultraviolet rather than reflecting it. The damage is self-propagating and irreversible. You cannot polish it off, and you cannot design around it with a better multilayer, because the absorbing material is the mirror itself.

This is why a bare aluminum mirror is a poor commercial product: its reflectance curve is not reproducible from one week to the next, and its handling tolerance is close to zero. Any supplier who quotes a UV aluminum reflectance is implicitly quoting a protected coating, whether or not they say so.

What the MgF2 overcoat actually buys, and what it costs

Thorlabs seals the aluminum under a magnesium fluoride layer. The manufacturer states the purpose plainly: the UV-enhanced aluminum coating has an overcoat of MgF2 to increase its average reflectance in the ultraviolet portion of the spectrum, and because bare aluminum is extremely delicate and susceptible to damage, that protective overcoat is layered over the aluminum to prolong the life of the mirror. Two mechanisms are being served at once, and it is worth separating them. The fluoride is transparent deep into the ultraviolet, so unlike the silicon dioxide used on visible-range protected aluminum, it does not itself become the absorber. And it is hard enough, and chemically inert enough, that the metal underneath stops reacting with the atmosphere.

The cost is a dielectric layer sitting on top of a metal, which means interference. The overcoat introduces a reflectance ripple across the band and adds a small absorption of its own. That is the honest reason the guaranteed figure here is 90 percent rather than the 97 percent a protected silver coating delivers in the visible and near infrared. Seven points of reflectance are being traded for a mirror that still has the same reflectance next year, and for a UV optic that is normally the right trade.

Ninety percent is a respectable number below 450 nm

Put the figure next to its own family. The visible-range protected aluminum coating, the workhorse mirror of every optical table, is specified at 90 percent average reflectance from 450 nm to 2 µm. In the ultraviolet, this mirror matches that number. Meanwhile the dielectric UV mirrors that reach 99 percent do so across a band measured in tens of nanometres, at a price per square millimetre several times higher, and with an angular acceptance that collapses as soon as the beam walks off axis. If the source is broadband, if it is an excimer line with fluorescence around it, if it is a frequency-tripled beam with residual pump still travelling with it, a flat 90 percent across 250 to 450 nm usually buys more usable photons than 99 percent across a 20 nm window.

Two damage thresholds that look similar and are not

The published pulsed thresholds are 0.25 J/cm² at 266 nm and 0.3 J/cm² at 355 nm, both at 10 ns and 10 Hz, but at spot diameters of 0.150 mm and 0.381 mm respectively. As fluence the two figures are within 20 percent of each other. As energy per pulse they are not close at all: the 266 nm test spot carries roughly 44 microjoules, while the 355 nm spot carries roughly 342 microjoules. Anyone who reads only the fluence and assumes the mirror tolerates the same pulse energy at both wavelengths will be overdriving the 266 nm case by nearly a factor of eight. The spot size is part of the specification, not a footnote.

The continuous-wave figures tell a similar story in a different currency: 300 W/cm at 1.064 µm with a 0.044 mm spot, and 500 W/cm at 10.6 µm with a 0.339 mm spot. Converted to total power on the stated spot, those become about 1.3 W and about 17 W. The second number is larger mostly because the test spot is nearly eight times wider, not because the coating is dramatically tougher in the far infrared.

Key Features

  • UV-enhanced aluminum with an MgF2 overcoat – specified across 250 to 450 nm with an average reflectance of 90 percent, and sealed against the oxide growth that destroys unprotected aluminum in air.
  • Fused silica substrate, 12.0 mm thick – a low coefficient of thermal expansion of 0.55 x 10-6 per degree C, and enough stiffness that a 2 inch aperture does not flex under a retaining ring.
  • Lambda/10 peak-to-valley at 633 nm – the figure is quoted at the helium-neon line rather than at a UV wavelength, and it applies over the clear aperture rather than across the full outside diameter.
  • 40-20 scratch-dig surface quality – a laser-grade cosmetic specification, appropriate for a mirror that will sit in a beam rather than behind a window.
  • 45.7 mm clear aperture – 90 percent of the 50.8 mm outside diameter, so a 40 mm beam can be steered without clipping.
  • Angle of incidence 0 to 45 degrees – usable both as a fold mirror and as a beamsplitter-style pickoff, though the reflectance curve shifts as the angle opens up.
  • Diameter tolerance +0.0 / -0.1 mm, thickness tolerance plus or minus 0.2 mm – tolerances that let the optic drop into a standard 2 inch mount without shimming.
  • Parallelism 3 arcmin or better – the wedge is small enough that a beam reflected from the back surface will not walk back into your source.
  • Part number laser engraved on the rear face – standard on Thorlabs optics from 1/2 inch upward, so a mirror pulled out of a drawer can be identified without a caliper and a reflectance curve.

Technical Specifications

Parameter Specification
Coating UV-enhanced aluminum with MgF2 overcoat
Specified wavelength range 250 – 450 nm
Average reflectance (Ravg) 90 percent
Substrate Fused silica
Substrate CTE 0.55 x 10-6 per degree C
Diameter 50.8 mm (2 in)
Diameter tolerance +0.0 / -0.1 mm
Thickness 12.0 mm (0.47 in)
Thickness tolerance plus or minus 0.2 mm
Clear aperture 90 percent of diameter, 45.7 mm
Surface flatness lambda/10 peak-to-valley at 633 nm
Surface quality 40-20 scratch-dig
Parallelism 3 arcmin or better
Angle of incidence 0 to 45 degrees
Marking Part number laser engraved on the back surface

Laser induced damage threshold, as published

Test condition Threshold Energy on that spot
266 nm, 10 ns, 10 Hz, spot 0.150 mm 0.25 J/cm² about 44 microjoules
355 nm, 10 ns, 10 Hz, spot 0.381 mm 0.3 J/cm² about 342 microjoules
1.064 µm, CW, spot 0.044 mm 300 W/cm about 1.3 W
10.6 µm, CW, spot 0.339 mm 500 W/cm about 17 W

Thorlabs is explicit that these damage values belong to the coating, not to the diameter: the threshold of a given coating is measured once and does not change when the same coating is deposited on a larger optic. The other half of that statement matters more in practice. The measurements are made on clean optics, and contamination on the surface lowers the threshold substantially. In the ultraviolet, where a fingerprint absorbs instead of transmitting, that penalty is larger than it is anywhere else in the spectrum.

Applications

Excimer and frequency-tripled sources

The 248 nm krypton fluoride line sits inside the specified band and is the single most common reason to buy this optic; the 355 nm third harmonic of Nd:YAG is the second. Both are pulsed, both are usually delivered as a beam with a residual fundamental still present, and both punish a mirror that has any absorption at all. A 90 percent average reflectance across the whole 250 to 450 nm window is what lets one optic handle the harmonic and whatever accompanies it.

Beam expansion and collimation in the ultraviolet

Ultraviolet beams are difficult to compress. Diffraction-limited spot size scales with wavelength, so a UV beam that has to travel a metre arrives with a divergence that a visible beam of the same waist would not have, and the usual remedy is to expand it early and collimate it well. That means large apertures. A 2 inch mirror with a 45.7 mm clear aperture gives room for an expanded beam plus alignment margin, and the 12 mm thickness keeps the surface figure stable when the optic is clamped.

Inspection, fluorescence and curing illumination

Where the source is a lamp or an LED rather than a laser, damage threshold is irrelevant and average reflectance is everything. Deuterium lamps, UV LEDs at 265 to 365 nm, fluorescence excitation paths and UV curing relays all benefit from a mirror that does not have to be re-characterised as it ages. The flat 90 percent curve also means the spectral shape of the illumination is preserved rather than modulated by a ripple.

Where this mirror is the wrong choice

Below 250 nm the guarantee ends. Above 450 nm the protected aluminum coating is cheaper and reaches further into the infrared. And if the beam is a single narrow line and the budget allows, a dielectric UV mirror will beat 90 percent by a wide margin over that line. The UV-enhanced aluminum mirror is the generalist of the ultraviolet, not the specialist.

Selection Guide

Three questions settle most UV mirror choices. What is the shortest wavelength in the beam? What is the longest? And is the source pulsed enough for damage threshold to matter?

  • Shortest wavelength between 250 and 450 nm, broadband source – this mirror. Nothing else in the family covers the band.
  • Shortest wavelength 450 nm or longer – the protected aluminum PF20-03-G01 covers 450 nm to 20 µm at 90 percent, and costs less for the same aperture.
  • Visible to near infrared with the highest possible reflectance – protected silver PF20-03-P01, at 97 percent from 450 nm to 2 µm and 95 percent beyond.
  • Infrared only, 800 nm and beyond – protected gold PF20-03-M01 at 96 percent, or the mid-infrared enhanced gold PF20-03-M02 at 98 percent above 2 µm.
  • Polarization must survive the reflection – unprotected gold PF20-03-M03, at the cost of a surface that cannot be cleaned.
  • Single CO2 line at 10.6 µm – the line-specific unprotected gold PF20-03-L01, at 99 percent.

One more question is worth asking before ordering: does the beam ever run at a steep angle? At 45 degrees the s and p reflectances of a metal coating separate, and the average figure quoted at near-normal incidence is no longer the number you will measure. If the fold is at 45 degrees and polarization matters, plan for a waveplate or accept the split.

Series Comparison

All seven coatings below are available on the same 50.8 mm, 12.0 mm fused silica substrate, so the comparison is purely a comparison of coatings. Values are the manufacturer’s specified averages.

Coating code Coating Band Ravg Relevance to UV work
-F01 UV enhanced aluminum 250 – 450 nm 90 percent The only coating in the family with a UV guarantee
-G01 Protected aluminum 450 nm – 20 µm 90 percent to 2 µm, 95 percent beyond No UV guarantee at all; starts where F01 stops
-P01 Protected silver 450 nm – 20 µm 97 percent to 2 µm, 95 percent beyond Highest visible reflectance, but silver absorbs in the UV
-M01 Protected gold 800 nm – 20 µm 96 percent Unusable in the UV; gold absorbs below 800 nm
-M02 MIR enhanced gold 2 – 20 µm 98 percent Far infrared only
-M03 Unprotected gold 800 nm – 20 µm 97 percent Far infrared only, and cannot be cleaned
-L01 Unprotected gold, line optimised 10.6 µm 99 percent Far infrared only

FAQ

Can this mirror be used at 248 nm, and can it be used at 193 nm?

Yes at 248 nm, no at 193 nm. The guaranteed band begins at 250 nm, and 248 nm is close enough to that edge that the coating is still operating in its designed region; the krypton fluoride line is one of the standard uses of this optic. At 193 nm you are outside the guarantee by a wide margin, the MgF2 overcoat and the aluminum beneath it both begin to absorb heavily, and the damage threshold falls away. An argon fluoride beam needs a dedicated deep-UV coating, not this one. If your system runs both 248 nm and 193 nm, they need two different mirrors.

Why is the reflectance only 90 percent when UV dielectric mirrors advertise 99 percent?

Because they are answering a different question. A dielectric stack can reach 99 percent, but only across a band of tens of nanometres and only near its design angle. This is a metal coating with a protective overcoat: it holds 90 percent across 200 nm of spectrum, at any angle from normal incidence to 45 degrees. For a single narrow line, the dielectric wins on reflectance. For a broadband or multi-line UV path, this mirror is the only one that covers the whole range without being swapped.

Is 0.25 J/cm² at 266 nm a lot or a little?

On the test spot, it is about 44 microjoules. That is a modest pulse. If your 266 nm beam carries more than that per pulse, you need to expand the spot so the fluence stays under the limit, which is one of the reasons a 2 inch mirror is specified rather than a half-inch one. Always compute fluence on your own beam diameter, not on the diameter of the optic.

Does the 12 mm thickness matter optically?

Not for the reflected beam, since the reflection happens at the front surface. It matters mechanically and thermally: a thicker substrate resists clamping distortion, holds figure under a heavy mount, and spreads heat laterally so a local hot spot does not become a local figure error. The penalty is mass and the need for a mount that accepts a 12 mm edge.

Can I clean this mirror with ordinary lens tissue and solvent?

The MgF2 overcoat is hard and is one of the more forgiving UV surfaces, but the aluminum underneath it is still a metal film, and the edge of the coating is where damage starts. Use reagent-grade acetone, methanol or isopropanol on lens tissue, drag rather than rub, work from the centre outward, and never press on a visible defect. If the contamination is a fingerprint, clean it before the next laser run rather than after; the absorption penalty in the ultraviolet is severe.

Will the reflectance hold at 45 degrees?

The specified average is a near-normal figure. At 45 degrees, s-polarised light reflects slightly better than the average and p-polarised light slightly worse, and the separation grows toward the short-wavelength end of the band. For a beam that must keep its polarisation through several folds, either stay near normal incidence or plan the polarisation budget explicitly.

Usage Precautions

  • Handle by the edge only. The coating is protected but thin; contact with a glove that has been resting on a bench transfers oils that absorb in the ultraviolet far more aggressively than they would in the visible.
  • Do not over-torque the retaining ring. A 2 inch, 12 mm optic is stiff, but a nylon-tipped set screw tightened against the barrel can still print a local figure error into a lambda/10 surface. Finger tight plus a quarter turn is the working rule.
  • Keep the coated face out of the beam dump. Back-scattered light from a dump can deposit ablation debris on the nearest optic; in UV systems that debris is often the initiator of a damage site.
  • Store in the original case, coated face up, nothing touching the surface. Stacked optics are the single most common cause of scratches that arrive before the first use.
  • Verify the part number on the back before installation. The UV, visible and infrared coatings in this family look identical under room light. A gold mirror installed where a UV mirror was intended will be discovered only when the beam power drops.
  • Respect the laser safety envelope. A 90 percent reflector sends 10 percent of the beam somewhere. In the ultraviolet that stray beam is both an eye hazard and an ozone source; enclose the path.

Disclaimer

The specifications in this page are transcribed from the manufacturer’s published data for the PF20-03-F01 and are provided for selection purposes. Damage thresholds are test values measured on clean optics under the stated conditions and are not a guarantee of survival in any particular system; actual performance depends on beam profile, pulse shape, repetition rate, spot size, surface contamination and mounting. Reflectance values are averages over the stated band and do not describe behaviour at a single wavelength or at a specific angle of incidence. Gaofei Laser is a distributor and integrator, not the manufacturer of this optic; where a value is critical to a design, request the current specification sheet before committing.

Contact Us

For a quotation, a stock check or help deciding between the UV, visible and infrared coatings in this family, contact Gaofei Laser:

Hotline: +86 159-2722-0467
Email: 859818709@qq.com
Website: www.soar-laser.cn

Send us the wavelength range, the beam diameter, the pulse energy or CW power and the angle of incidence, and we will confirm whether the PF20-03-F01 is the right coating or point you to the one that is.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF20-03-F01 Ø50.8 mm (2 in) UV-Enhanced Aluminum Mirror, 250 – 450 nm”

Your email address will not be published. Required fields are marked *

中文EN