QQ: 859818709

Thorlabs PF07-03-F01 Ø19.0 mm UV-Enhanced Aluminum Mirror, 250-450 nm

Thorlabs PF07-03-F01 Ø19.0 mm UV-Enhanced Aluminum Mirror, 250-450 nm

Price on request
Category:

Description

Product Overview

The Thorlabs PF07-03-F01 is a Ø19.0 mm plano mirror carrying a UV-enhanced aluminium coating on a fused silica substrate, specified from 250 to 450 nm at an average reflectance above 90%. Everything about the part is ordinary except the film: a 6.0 mm thick disc, λ/10 peak-to-valley figure at 633 nm, 40-20 scratch-dig surface quality, parallelism held within 3 arcmin. The coating is what makes it the one member of this group that works in the ultraviolet at all.

Metal selection below 450 nm is not a matter of taste. Silver has its plasma edge in the deep ultraviolet and its reflectance falls away steeply under roughly 350 nm, so a silver mirror that looks excellent at 532 nm is a mediocre reflector at 355 nm and a poor one at 266 nm. Gold is worse: its interband transitions absorb everything shorter than the visible, which is why a gold mirror looks yellow rather than white. Aluminium is the only metal with useful ultraviolet reflectance, and even aluminium is compromised in practice, because the film oxidises in air and the native oxide absorbs exactly where the ultraviolet work happens. The UV-enhanced process deposits the aluminium so that this oxide stays thin, then caps it with a magnesium fluoride overcoat. MgF₂ is used here rather than the silica that seals the protected coatings, because silica begins to absorb in the deep ultraviolet while magnesium fluoride is still transparent there.

The Ø19.0 mm diameter is not arbitrary. It is the format Thorlabs built its Polaris fixed optic mount around: the POLARIS-19S50/M takes a 6 mm thick, 19 mm optic in a monolithic flexure arm that contacts the mirror at three axial points, giving a Ø1 inch mounting footprint with a clear aperture larger than a Ø1/2 inch optic can offer. For ultraviolet work that combination matters more than elsewhere. Ultraviolet beams are hard to see, alignment is usually done against a fluorescent card or a faint spot, and the last thing wanted is a mount that shifts when the optic comes out for inspection. A fixed mount with a repeatable seat removes that variable, and the 6.0 mm substrate is thick enough for the flexure arm to hold without bending it.

Key Features

  • Magnesium fluoride overcoat: transparent in the deep ultraviolet, where the silica seal used on the protected coatings would already be absorbing
  • Above 90% average from 250 to 450 nm: the only coating in this 19 mm group specified below 450 nm, and the reason the page exists
  • Nanosecond thresholds at both harmonics: 0.25 J/cm² at 266 nm and 0.3 J/cm² at 355 nm, both measured with 10 ns pulses at 10 Hz
  • Not a cleanable optic: the aluminium layer is soft and the MgF₂ cap is thin and mildly hygroscopic, so contamination is blown off with dry gas rather than wiped
  • Ø19.0 mm x 6.0 mm fused silica: λ/10 figure at 633 nm, 40-20 scratch-dig, clear aperture 90% of the diameter
  • Metallic, therefore angle-tolerant: reflectance changes gradually with incidence, so one part serves a 45 degree fold and a near-normal pickoff in the same layout

Technical Specifications

Model PF07-03-F01
Coating UV-enhanced aluminium
Overcoat Magnesium fluoride (MgF₂)
Wavelength range 250 nm – 450 nm
Average reflectance above 90% from 250 to 450 nm
Substrate Fused silica
Diameter Ø19.0 mm (0.75 in)
Diameter tolerance +0.0 mm / -0.1 mm
Thickness 6.0 mm (0.24 in)
Thickness tolerance +/-0.2 mm
Clear aperture 90% of diameter, about Ø17.1 mm
Surface flatness λ/10 peak to valley at 633 nm
Surface quality 40-20 scratch-dig
Parallelism at most 3 arcmin
Pulsed damage threshold 0.25 J/cm² at 266 nm (10 ns, 10 Hz, Ø0.150 mm); 0.3 J/cm² at 355 nm (10 ns, 10 Hz, Ø0.381 mm)
CW damage threshold 300 W/cm at 1.064 µm (Ø0.044 mm); 500 W/cm at 10.6 µm (Ø0.339 mm)
Mount POLARIS-19S50/M fixed monolithic mount for Ø19 mm optics
Cleanable No, dry gas only
Source Thorlabs official series specification table

Applications

The coating fixes the band, so the applications are the ones where a beam below 450 nm has to be turned and a dielectric stack is either too expensive at that wavelength or too narrow for the job.

  • Third harmonic routing: pulling 355 nm out of a Nd:YAG or similar path after the tripler, where the optic sees nanosecond pulses and has to hold its figure under them
  • Ultraviolet beam conditioning: folding a collimated 266 or 355 nm beam between the collimator and the focusing lens, where a λ/10 surface keeps the focal spot from growing
  • Ultraviolet interferometry and wavefront metrology: any folded path in which the reflection itself must not add aberration to the test beam
  • Photoluminescence and fluorescence excitation: routing a short-wavelength pump to the sample close to the collection optics, where a 6 mm substrate keeps the geometry compact
  • Mixed harmonic paths: a beam carrying 355 nm and 532 nm together, where a metal coating serves both and a dielectric design would have to be centred on one of them

Selection Guide

  • Stay inside 250 to 450 nm: reflectance above 450 nm is not specified for this coating. It will reflect, but nothing is guaranteed, and a 532 nm beam belongs on the protected aluminium or protected silver page instead
  • Decide the cleaning regime before the budget: if the optic will be wiped on a production line, this is the wrong film whatever the wavelength. Either choose a protected coating and accept lower ultraviolet reflectance, or design the holder so the mirror is never touched
  • Size the aperture to the beam, not to the mount: the clear aperture is 90% of 19.0 mm, roughly 17 mm. Keep the 1/e² beam inside about 12 mm so that diffraction from the edge does not appear as haze in a dark ultraviolet image
  • Compare against a dielectric when the band is narrow: a dielectric coating can beat 99% across a 20 nm window, but it is angle sensitive and expensive at 266 nm. The metal coating wins when the wavelength moves or the incidence angle varies
  • Plan for storage: magnesium fluoride is mildly hygroscopic. A mirror installed once a year should live in a desiccator between uses rather than on an open shelf in a humid lab

Series Comparison

The five Ø19.0 mm coatings share one substrate, one thickness and one mount, so the comparison is purely a question of band and handling. This page is the short-wavelength end of that table.

Item Coating Wavelength range Average reflectance Overcoat Cleanable
PF07-03-F01, this page UV-enhanced aluminium 250 – 450 nm above 90% MgF₂ No
PF07-03-G01 Protected aluminium 450 nm – 2 µm (above 90%); 2 – 20 µm (above 95%) 90% / 95% SiO₂ Yes
PF07-03-M01 Protected gold 800 nm – 20 µm 96% Dielectric Yes
PF07-03-M02 MIR-enhanced gold 2 – 20 µm 98% average, 95% absorption-weighted Dielectric Yes
PF07-03-P01 Protected silver 450 nm – 2 µm (above 97%); 2 – 20 µm (above 95%) 97% / 95% SiO₂ Yes

The same coating is stocked on two smaller substrates for layouts that cannot take 19 mm: a Ø1/2 inch UV-enhanced aluminium mirror for standard 12.7 mm hardware, and a Ø7.0 mm version for the MK7 mini-series mount. An uncoated Ø19 mm fused silica blank is available if the coating is to be applied elsewhere.

FAQ

Why not use a silver mirror at 355 nm? Because silver stops reflecting there. Its plasma edge sits in the deep ultraviolet and the reflectance curve falls steeply below about 350 nm, so the same 97% that makes a silver mirror attractive at 532 nm is gone by 355 nm. Aluminium is the only metal with useful reflectance in that region.

Can this mirror be cleaned with solvent? No. The aluminium film is soft and the magnesium fluoride cap is thin, so a solvent and tissue wipe that is routine on a protected gold mirror will damage this coating. Dust is removed with clean dry nitrogen or filtered air, and an optic contaminated beyond that is replaced rather than cleaned.

Why magnesium fluoride rather than the silica used on the other coatings? Because silica absorbs in the deep ultraviolet. A silica seal is durable and cheap and works well over the visible and infrared, but it would defeat the purpose of a coating specified down to 250 nm. Magnesium fluoride stays transparent further into the ultraviolet, at the cost of being softer and mildly hygroscopic.

What happens if the beam is 532 nm? The mirror will reflect it, but the reflectance is not specified above 450 nm, so no number can be quoted and no link budget should be built on it. For 532 nm choose the protected silver or protected aluminium item, both of which are specified across that wavelength.

Are the two published thresholds for different harmonics? Yes. One is 0.25 J/cm² at 266 nm and the other 0.3 J/cm² at 355 nm, both with 10 ns pulses at 10 Hz. The 355 nm figure is the higher of the two, which reflects how the coating absorbs at each wavelength rather than any difference in the substrate.

Will a Ø19 mm mirror fit a standard 1/2 inch mount? No. Ø19.0 mm is 0.75 inch, not 12.7 mm, and a 6.0 mm substrate is far thicker than the 1/2 inch standard. It fits the POLARIS-19S50/M and other mounts made for 19 mm optics; forcing it into a 12.7 mm holder leaves it unseated and distorts the figure.

Usage Precautions

  • Handle by the rim: finger cots or powder-free gloves, edge contact only. Skin oils absorb strongly in the ultraviolet, so a fingerprint that would be cosmetic on a gold mirror becomes a hot spot that grows under illumination
  • Dry cleaning only: blow off particles with clean dry gas. Do not drag a lens tissue across the surface and do not use acetone, methanol or any polymer film on this coating
  • Control humidity in storage: magnesium fluoride takes up water slowly. Keep the mirror in its case with desiccant, and let a cold optic reach room temperature before opening the case so that condensation does not form on the film
  • Do not over-clamp: the flexure arm or retaining ring should just hold the optic. A 6 mm substrate will bend under a heavy ring, and a bent mirror has lost the λ/10 figure it was bought for, which appears as astigmatism in the reflected beam
  • Watch the energy density, not the laser power: compare the fluence at the mirror surface with the published 266 or 355 nm threshold for the actual pulse length. Scatter from the coating edge and from surface contamination usually starts damage before the nominal beam does
  • Avoid direct back reflection: tilt the mirror a degree or two off normal where the layout allows, so the return does not re-enter the laser cavity and destabilise it

Disclaimer

Specifications on this page are compiled from Thorlabs official published material and are provided as a selection reference. The current official specification sheet governs; specifications and appearance may change without notice. Price and lead time are quoted by our sales team on request.

Contact Us

Changsha Soar Laser Equipment Co., Ltd. supplies Thorlabs optics with local stock, technical support and export documentation. For coating selection, quantity pricing or a substitute recommendation, contact us on +86 159 2722 0467, by email at 859818709@qq.com, or through www.soar-laser.cn.

Reviews

There are no reviews yet.

Be the first to review “Thorlabs PF07-03-F01 Ø19.0 mm UV-Enhanced Aluminum Mirror, 250-450 nm”

Your email address will not be published. Required fields are marked *

中文EN